West Coast Regional Sales Manager
- FMA
- The Fabricator
- FABTECH
- Canadian Metalworking
Categories
- Additive Manufacturing
- Aluminum Welding
- Arc Welding
- Assembly and Joining
- Automation and Robotics
- Bending and Forming
- Consumables
- Cutting and Weld Prep
- Electric Vehicles
- En Español
- Finishing
- Hydroforming
- Laser Cutting
- Laser Welding
- Machining
- Manufacturing Software
- Materials Handling
- Metals/Materials
- Oxyfuel Cutting
- Plasma Cutting
- Power Tools
- Punching and Other Holemaking
- Roll Forming
- Safety
- Sawing
- Shearing
- Shop Management
- Testing and Measuring
- Tube and Pipe Fabrication
- Tube and Pipe Production
- Waterjet Cutting
Industry Directory
Webcasts
Podcasts
FAB 40
Advertise
Subscribe
Account Login
Search
Band sawing structurals
Cutting tips that lead to better welds
- By Dirk Herzog
- May 15, 2013
- Article
- Sawing
When band saw cutting I-beam, square, and round tubing, straight cuts are crucial to preparing the part properly for welding. Parts with crooked cuts make welding difficult, to say the least, and as a result, welders often must use a filler or additional welding wire to fill the gap left by the uneven edge. In more severe cases, the parts with uneven cuts may have to be recut or scrapped altogether, which is both costly and time-consuming.
If you are performing structural cuts with a band saw, consider these tips to help ensure that edges are straight and that welders can join parts easily and efficiently. Keep in mind the importance of routine maintenance on the band saw machine. If a machine has problems with its feed system or its variable-speed system, it will negatively affect the life of the band saw blade.
Know the Sawing Parameters
The best way to ensure the cuts you make will be straight is to set your sawing parameters correctly. Set the machine to the correct blade speed and cut rate for the material being cut. As a rule, slow the blade for tough material and increase speed for softer material.
Also, check to make sure the conveyor rollers that hold the material are aligned properly. Rollers that are out of alignment can lead to crooked cuts.
Set the Tension Properly
Use a gauge to measure and set the tension on the blade in the band saw machine. Most band saws work best with the blade tension set to a minimum of 25,000 PSI or a maximum of 32,000 PSI. Anything less than 25,000 PSI leads to poor beam strength, band fatigue, or crooked cuts. Tensions set to 32,000 PSI or more can break the band, crack the gullets, or wear out the machine bearings.
Cut From the Back of the Weld Seam
For applications that involve cutting through a weld seam on tubing, it is easier and more efficient for the band saw blade to enter the material from the back of the weld seam. Cutting directly into the weld seam serves as a shock point to the blade teeth and often results in shorter blade life or teeth strippage.
Secure the Bundles
When band sawing bundles of material, it is best to strap down the entire bundle or tack weld the ends of the bundle to prevent any pieces from moving. If the individual pieces vibrate or move during the cutting process, there is a possibility that the teeth will strip.
Use Proper Lubrication
The proper amount of cutting lubricant, also known as coolant, will help extend blade life. Band saws use a flood-coolant or a mist system to lubricate the blade. Not only does lubrication help maximize blade life, it also helps minimize the buildup of metal chips that result when the material is cut. Coolant should wash over the blade as it enters and exits the cut. Although the coolant is recirculated and used continuously throughout the cutting process, be sure to replace water that evaporates from the mixed solution.
Breakin New Blades
Be sure to break in new band saw blades before you ramp them up to full-speed cutting. This practice will hone the teeth and extend blade life. The best way to break in new bimetal blades is by reducing the normal feed rate by half during this initial period. The band speed isn’t what breaks teeth during blade break-in; it’s the pressure an excessive feed rate produces that is most damaging.
To break in your bimetal saw blade, multiply the recommended blade speed by 25 percent, and cut that number of square inches. Be sure to run the blade at 50 percent of the recommended blade feed rate. Once you approach the end of the break-in period, gradually bring your band saw feed rate up to normal.
Use the Right Blade
The right band saw blade makes all the difference when cutting structurals, where the desired outcome is a clean, straight cut that simplifies weld prep applications. Be sure to choose a blade that can withstand the stresses of structural cutting, produce a smooth finish, and ensure maximum blade life. Also, optimal tooth geometry is key to creating faster cutting rates, which increase productivity.
About the Author
Dirk Herzog
135 Intervale Road
Fitchburg, MA 01420
978-424-0100
About the Publication
Related Companies
subscribe now
The Welder, formerly known as Practical Welding Today, is a showcase of the real people who make the products we use and work with every day. This magazine has served the welding community in North America well for more than 20 years.
start your free subscription- Stay connected from anywhere
Easily access valuable industry resources now with full access to the digital edition of The Fabricator.
Easily access valuable industry resources now with full access to the digital edition of The Welder.
Easily access valuable industry resources now with full access to the digital edition of The Tube and Pipe Journal.
Easily access valuable industry resources now with full access to the digital edition of The Fabricator en Español.
- Podcasting
- Podcast:
- The Fabricator Podcast
- Published:
- 05/14/2024
- Running Time:
- 62:12
Cameron Adams of Laser Precision, a contract metal fabricator in the Chicago area, joins the podcast to talk...
- Trending Articles
Connecticut students compete in Maritime Welding Competition
Welding power source’s modes designed to help optimize performance
Building a successful welding program from the ground up
Torch made for welding thin, conductive sheet metal
Welding jacket designed for protection, comfort
- Industry Events
Laser Welding Certificate Course
- May 7 - August 6, 2024
- Farmington Hills, IL
World-Class Roll Forming Workshop
- June 5 - 6, 2024
- Louisville, KY
Advanced Laser Application Workshop
- June 25 - 27, 2024
- Novi, MI
Precision Press Brake Certificate Course
- July 31 - August 1, 2024
- Elgin,