- FMA
- The Fabricator
- FABTECH
- Canadian Metalworking
Categories
- Additive Manufacturing
- Aluminum Welding
- Arc Welding
- Assembly and Joining
- Automation and Robotics
- Bending and Forming
- Consumables
- Cutting and Weld Prep
- Electric Vehicles
- En Español
- Finishing
- Hydroforming
- Laser Cutting
- Laser Welding
- Machining
- Manufacturing Software
- Materials Handling
- Metals/Materials
- Oxyfuel Cutting
- Plasma Cutting
- Power Tools
- Punching and Other Holemaking
- Roll Forming
- Safety
- Sawing
- Shearing
- Shop Management
- Testing and Measuring
- Tube and Pipe Fabrication
- Tube and Pipe Production
- Waterjet Cutting
Industry Directory
Webcasts
Podcasts
FAB 40
Advertise
Subscribe
Account Login
Search
Applications: Carbide circular cold saw brings turbulator production back in-house
Situation
Turbulator Co., located in Oklahoma City, Okla., makes turbulators for the cementing phase of the oil well drilling process. To produce these metal cylinders with blades welded to the outer surface, the company makes about 700,000 high-tolerance, precision cuts per year.
“With the volume we’re doing, we have to maintain a throughput rate that can make your head spin,” explained Jackie McHenry, president. “Finding metal cutting saws that can handle the load has been a challenge.
Until recently the company was using two automated band saws to process all the cutting jobs, but it often had to farm out work to job shops to keep up with production demands. As customer delivery schedules grew tighter and more new orders were entered, McHenry decided that approach wasn’t enough to remain competitive while maintaining or improving quality.
“We absolutely needed the saw to be able to perform high-speed, precision cutting with minimal operator monitoring on a near 24/7 basis."
Resolution
The company acquired a Behringer Eisele HCS 160 carbide circular cold saw for high-speed cutting of metal barstock. The fully automatic saw is designed for cutting high-alloy, heat-resistant steels.
Configured for workpiece diameters up to 160 mm, the saw delivers speeds of 20 to 250 RPM to accommodate wet and dry sawing applications. Its rigid frame helps dampen vibrations, and a new blade guide features a blade vibration absorber design.
This saw uses multifluid cooling technology to prevent heat transfer to product during mass cutting applications. Its flood coolant system enables rapid cutting over long periods of time with few interruptions. Operators don’t need to keep checking the work for heat buildup, so unattended operation is increased. Additionally, the saw has a vortex air blowing system to help improve cutting temperature control and to ensure material stays free of liquid when required.
The single saw has replaced the original two band saws, and the company no longer relies on outside machine shops for cutting.
“The saw helped us shorten our supply chain," said McHenry, “and in the oil drilling business, that is an important step toward being successful."
Related Companies
subscribe now
The Fabricator is North America's leading magazine for the metal forming and fabricating industry. The magazine delivers the news, technical articles, and case histories that enable fabricators to do their jobs more efficiently. The Fabricator has served the industry since 1970.
start your free subscription- Stay connected from anywhere
Easily access valuable industry resources now with full access to the digital edition of The Fabricator.
Easily access valuable industry resources now with full access to the digital edition of The Welder.
Easily access valuable industry resources now with full access to the digital edition of The Tube and Pipe Journal.
Easily access valuable industry resources now with full access to the digital edition of The Fabricator en Español.
- Podcasting
- Podcast:
- The Fabricator Podcast
- Published:
- 05/07/2024
- Running Time:
- 67:38
Patrick Brunken, VP of Addison Machine Engineering, joins The Fabricator Podcast to talk about the tube and pipe...
- Trending Articles
White House considers China tariff increases on materials
A deep dive into a bleeding-edge automation strategy in metal fabrication
A visit to Automate 2024 reveals the future might be now
Majestic Steel Arkansas fully operational
Rivian to expand Illinois facility to manufacture midsized SUV
- Industry Events
Laser Welding Certificate Course
- May 7 - August 6, 2024
- Farmington Hills, IL
World-Class Roll Forming Workshop
- June 5 - 6, 2024
- Louisville, KY
Advanced Laser Application Workshop
- June 25 - 27, 2024
- Novi, MI
Precision Press Brake Certificate Course
- July 31 - August 1, 2024
- Elgin,