- FMA
- The Fabricator
- FABTECH
- Canadian Metalworking
Categories
- Additive Manufacturing
- Aluminum Welding
- Arc Welding
- Assembly and Joining
- Automation and Robotics
- Bending and Forming
- Consumables
- Cutting and Weld Prep
- Electric Vehicles
- En Español
- Finishing
- Hydroforming
- Laser Cutting
- Laser Welding
- Machining
- Manufacturing Software
- Materials Handling
- Metals/Materials
- Oxyfuel Cutting
- Plasma Cutting
- Power Tools
- Punching and Other Holemaking
- Roll Forming
- Safety
- Sawing
- Shearing
- Shop Management
- Testing and Measuring
- Tube and Pipe Fabrication
- Tube and Pipe Production
- Waterjet Cutting
Industry Directory
Webcasts
Podcasts
FAB 40
Advertise
Subscribe
Account Login
Search
Precision sheet metal bending and the V groove
V-grooving makes the impossible bend possible
- By Steve Benson
- May 22, 2019
- Article
- Bending and Forming
Question: I have been working in job shops for many years, but until recently I had never heard of V-grooving for producing sheet metal parts. Everything I’ve read on the topic, which isn’t much, talks about the advantages of V-grooving but not so much about what goes on after these grooves are in the flat part. Do you still need a press brake, or is the part formed by hand? How is the inside radius produced in this type of bend, and how is the bend allowance and bend deduction calculated? When, how, and where would I use V-grooving, and what kind of parts would benefit from it?
Answer: I first came across the concept of grooving back in the 1960s, but that’s another story best left untold. Fast-forward 40 years and grooving now has a much different interpretation, at least when it comes to manufacturing sheet metal and plate parts.
Grooving the Small
I first encountered metal grooving about 10 years ago while producing some extremely small parts in my shop. The materials were thinner than 0.012 inch, with a dimensional tolerance of ±0.0015 in. and an angular tolerance of ±0.5 degree. For those thicknesses and materials, photo etching was the best option for producing the flat. Photo etching did more than just cut the perimeter of the piece. It also gave me the ability to use half-etch lines to establish the bend lines.
In the photo etching process, a laminate is secured to both sides of the sheet. The laminate has cutouts where the laminate is missing, exposing the metal underneath. Sprayed acid eats away at the exposed metal to produce the edges of features and the outer edge of the part. For the half-etch bend lines, only one cut laminate is placed on one side of the workpiece—on the surface of the material that will be the inside of the bend radius, eating away only half of the material thickness while establishing the location and direction of the bend.
For a given work order I received as many pieces as would fit on a 12- by 18-in. sheet. The concept and process worked out well on this small scale. These parts were gold-plated after forming, which left no sign that the half-etch line was even there. Note, the photo etch process does not work with all material types.
Grooving on a Larger Scale
Outside the world of photo etching, we define V-grooving for bending as a method of establishing the bend line and bend angle using grooves cut along the bend line. It’s also known as score-folding, V-cutting, and back-scoring. The grooving process, performed by a separate cutting machine, produces a V-cut located at the bend line. After groove-cutting, the bend can be completed at the press brake or even by hand. At the press brake, the operator can bend the grooved metal into various angles and shapes using off-the-shelf or custom tools.
V-grooving works best in (but is not limited to) material thicknesses from 0.031 to 0.236 in. It works with ferrous and nonferrous metals and other materials, including plastics, aluminum, composite plate, brass, bronze, copper, gold, silver, zinc, PVD-coated colored stainless steel, various stainless steel grades, and mild steel.
Why V-groove?
Some parts have features that traditional press brake bending methods simply cannot produce. When air forming sheet metal on a press brake, the punch pushes material into the die space. During forming, the sheet goes from the elastic state to its plastic state, where the sheet stays bent. The bend angle is set as a function of the depth of penetration into the die space, with the inside bend radius nearly equal to the material thickness, depending on the die width.
The behavior of the neutral axis is central to sheet metal bending. In the flat condition, the neutral axis is in the middle of the material thickness. During bending, compressive stresses occur on the inside of the bend, toward the inside bend radius, while expansion occurs toward the outside radius. These stresses shift the neutral axis toward the inside surface of the bend.
That shifting of the neutral axis produces the elongation we see when a sheet metal or plate part is bent. Remember that the flat is always smaller than the sum total of the outside dimensions of the finished piece.
Shortcomings of Traditional Bending
Lateral tensile stress on the outside bend radius often leads to discoloration seen on the outside of the bend—something unacceptable for an architectural application. V-grooving the sheet or plate reduces thickness at the bend line, which in turn reduces elongation and subsequent deformation caused by the lateral tensile force during bending.
When long, narrow flanges are bent on a press brake, deformation occurs from the applied compressive forces across the width of the bend. This deformation forces the material to elongate lengthwise (parallel to the bend line), convexing the edge of the bend at both ends.
At the same time, the outside bend radius, under tensile stress, causes the part to elongate slightly in the width direction (perpendicular to the bend line). This causes the outside bend radius to “pull in” somewhat, creating a center-concave condition. The larger the deformation, the more pronounced the center-concave condition becomes on the outside radius. For most parts this concaved area is of no consequence, but in an architectural application, it’s a big issue as it changes the look of the finished piece.
Because V-grooving reduces the thickness of the material at the bend line, you will see less of this concaving that results in straightness errors; often the outside radius becomes so small, concaving just isn’t an issue.
In conventional air bending, you’ll achieve the best results when you get as close as you can to having a one-to-one relationship between the inside bend radius and the material thickness—a perfect bend. However, depending on the material type and temper, you might need what’s effectively a zero-radius bend. And you still need to leave a smooth outside surface on the finished piece.
Sometimes a part might call for a radius that’s producible with a traditional air form, and a skilled operator could certainly produce these kinds of bends. But there are so many thicknesses and tensile variations within the tolerance zone for a particular gauge of sheets. Achieving consistent parts over time isn’t easy, and material inconsistencies at the press brake can result in variations in the bend angle, inside radius, and dimension.
Hence the advantage of thinning the material at the bend line with V-grooving and the subsequent reduction in the bend radius. Thinning the material at the bend line does weaken the bend, but if the resulting (lower) bend strength meets the job requirements, then it should be a viable technique for producing crisp, clean, and consistent bend dimensions and angles. V-grooving also will improve notch accuracy and the look of the finished part.
Architectural Advantages
The method works well for architectural fabrications. It can make decorative surfaces easy to manufacture for projects such as bank lobbies, hotels, airports, restaurants, shopping malls, and even kitchen equipment where finish and overall look are the primary goals. Manufacturers of sheet metal parts for decorative architectural panels, wall systems, and other aesthetic components often use V-grooving to produce sharp corners in panels that, once interlocked and mounted, give the appearance of being a seamless unit.
The process produces a very small bend radius that meets demands for specific jobs. The small bend radius also will lack excessive die marks that you would have from a traditional coining or bottoming operation.
In large or thick panels, V-grooving tends to reduce oil canning (waviness) in the metal surface, unlike traditional forming methods that introduce or amplify the oil canning and similar conditions like wrinkling and buckling.
Ordinarily, if you go too small with the inside radius for a forming operation, you’ll end up with cracking on the outside surface of the bend. But V-grooving allows the manufacturer of an architectural workpiece to meet critical requirements of a small inside radius while producing parts without the bend marks of traditional forming. Dimensional accuracy is spot-on, the look of the finished piece is topnotch, and bend angle accuracy is excellent.
Bending with V-grooving also reduces the straightness deviations of the radius edge on long and narrow pieces. The best part is, even complicated shapes can be produced at the press brake using standard acute tools.
Fooling a Professional
Again, V-grooving significantly reduces the material thickness at the bend line. A typical application might entail some prepainted aluminum that a shop needs to form without crazing (small cracks) on the outside of the bend. Conventional air bending with a press brake produces a relatively large outside radius—again, because the material outside the neutral axis is expanding. However, the surface paint doesn’t stretch well, hence the crazing on the outside of the bend. V-grooving can reduce the material thickness at the bend line by half, from 0.080 to 0.040 in., which allows for a clean, tight bend radius.
Nevertheless, thinning the material reduces the distance from the outside bend radius to the neutral axis, and this makes the process finicky at best. The bend naturally wants to occur in the center of the V-groove, so if you want to make minor adjustments to your backgauges for the bend location, the V-groove does not always cooperate. Also, bend angle adjustments don’t work quite as well as you’d think, especially if your material thickness varies.
The V-grooving process itself also can be a challenge. It will take some time to achieve the necessary depth of understanding to apply all the possibilities V-grooving presents. And though a machined groove looks nice, in many cases it can be a very slow and expensive addition to a bending process.
All that said, when the grooved bend is completed, it has a visibly tighter and cleaner outside bend radius that would easily fool a professional into believing that you were working with lighter-gauge material.
Of course, to fool a professional, you need to know what you’re doing. The V-groove and bending process has a plethora of details you need to consider. What kind of machine and cutting tool do you use to make the groove? What angle should that groove be? What are the springback considerations? And how does that V-groove affect your bend calculations? Stay tuned. We’ll cover all this and more next month.
About the Author
Steve Benson
2952 Doaks Ferry Road N.W.
Salem, OR 97301-4468
503-399-7514
Related Companies
subscribe now
The Fabricator is North America's leading magazine for the metal forming and fabricating industry. The magazine delivers the news, technical articles, and case histories that enable fabricators to do their jobs more efficiently. The Fabricator has served the industry since 1970.
start your free subscription- Stay connected from anywhere
Easily access valuable industry resources now with full access to the digital edition of The Fabricator.
Easily access valuable industry resources now with full access to the digital edition of The Welder.
Easily access valuable industry resources now with full access to the digital edition of The Tube and Pipe Journal.
Easily access valuable industry resources now with full access to the digital edition of The Fabricator en Español.
- Podcasting
- Podcast:
- The Fabricator Podcast
- Published:
- 05/14/2024
- Running Time:
- 62:12
Cameron Adams of Laser Precision, a contract metal fabricator in the Chicago area, joins the podcast to talk...
- Trending Articles
Why employee-owned companies make sense in manufacturing
What software automation means for custom fabrication
Nucor’s weekly steel price announcement continues to rattle markets
Press brakes, panel benders, and flat blank calculations
Educating, rather than just training, tomorrow's workforce
- Industry Events
Laser Welding Certificate Course
- May 7 - August 6, 2024
- Farmington Hills, IL
World-Class Roll Forming Workshop
- June 5 - 6, 2024
- Louisville, KY
Advanced Laser Application Workshop
- June 25 - 27, 2024
- Novi, MI
Precision Press Brake Certificate Course
- July 31 - August 1, 2024
- Elgin,