SW-95
Specifications
Model | SW-95 |
Operators | Dual |
Punch - U.S. Tons | 95 |
Punch - Std. Dia (in.) | 1.062 x 8.75 |
Punch - Max Dia. (In.) | 2 x .5 |
Punch - Throat Depth (In.) | 16 |
Shear - Shear Blade length (in.) | 16.125 |
Shear - Angle, 90 deg. | 5.125 x 5.125 x .5 |
Shear - Angle, 45 deg. | |
Shear - Channel | |
Shear - Flat Bar | 16 x .75 |
Shear - Rod, Round | 1.375 |
Shear - Rod, Square | 1.75 |
Notcher - Pipe Sch. 40 (in.) | 4 |
Notcher - Angle, 90 degree | |
Notcher - Rectangle | 2 x 3.5 x .5 |
Notcher - Vee | 5.75 x 5.75 x .375 |
Brake - Rated in U.S. Tons | 95 |
Automatic Positioning Table - S(Standard) O(Optional) N(Not Offered) | |
Automatic Positioning Table - X Travel (in.) | |
Automatic Positioning Table - Y Travel (in.) |
Baileigh Industrial Inc.
P.O. Box 531
1625 Dufek Drive
Manitowoc, WI 54221
Phone: 920-684-4990
Fax: 920-684-3944
baileigh.com
P.O. Box 531
1625 Dufek Drive
Manitowoc, WI 54221
Phone: 920-684-4990
Fax: 920-684-3944
baileigh.com