Regional Sales Specialist
- FMA
- The Fabricator
- FABTECH
- Canadian Metalworking
Our Publications
Categories
- Additive Manufacturing
- Aluminum Welding
- Arc Welding
- Assembly and Joining
- Automation and Robotics
- Bending and Forming
- Consumables
- Cutting and Weld Prep
- Electric Vehicles
- En Español
- Finishing
- Hydroforming
- Laser Cutting
- Laser Welding
- Machining
- Manufacturing Software
- Materials Handling
- Metals/Materials
- Oxyfuel Cutting
- Plasma Cutting
- Power Tools
- Punching and Other Holemaking
- Roll Forming
- Safety
- Sawing
- Shearing
- Shop Management
- Testing and Measuring
- Tube and Pipe Fabrication
- Tube and Pipe Production
- Waterjet Cutting
Industry Directory
Webcasts
Podcasts
FAB 40
Advertise
Subscribe
Account Login
Search
Dan Hernandez
Miller Electric Mfg. Co.
1635 W. Spencer St.
Appleton, WI 54912
920-734-9821
- From The Fabricator
Better preps, better pipe welds
- By Dan Hernandez
- Aug 9, 2017
- Tube and Pipe Fabrication
- Article
Following specified pipe welding procedures and ensuring proper weld preparation can save significant time and money and ultimately improve productivity of the entire operation.
Advanced GMAW processes help in welding P91
- By Dan Hernandez and David Benson
- May 26, 2016
- Tube and Pipe Fabrication
- Article
Alloy P91 has excellent high-temperature strength and creep resistance, making it a favored alloy for piping systems for power boilers and other applications that work at elevated temperatures and pressures. The conventional welding processes, gas tungsten arc welding and shielded metal arc welding, do a good job on P91, but modified gas metal arc welding (GMAW) processes and flux-cored arc welding (FCAW) have deposition rates three to four times faster.
- Podcasting
- Podcast:
- The Fabricator Podcast
- Published:
- 05/07/2024
- Running Time:
- 67:38
Patrick Brunken, VP of Addison Machine Engineering, joins The Fabricator Podcast to talk about the tube and pipe...
- Trending Articles
Young fabricators ready to step forward at family shop
Material handling automation moves forward at MODEX
Connecticut students compete in Maritime Welding Competition
A deep dive into a bleeding-edge automation strategy in metal fabrication
White House considers China tariff increases on materials
- Industry Events
Laser Welding Certificate Course
- May 7 - August 6, 2024
- Farmington Hills, IL
World-Class Roll Forming Workshop
- June 5 - 6, 2024
- Louisville, KY
Advanced Laser Application Workshop
- June 25 - 27, 2024
- Novi, MI
Precision Press Brake Certificate Course
- July 31 - August 1, 2024
- Elgin,
- Upcoming Webcasts
Navigating Change: The Manufacturer’s Guide to Change Management with ERP Implementation
- May 16, 2024
- Sponsored
- Presented By: ECI Software Solutions, M1
Managing Dangerous Dusts from Metalworking
- June 26, 2024
- Sponsored
- Presented By: Camfil Air Pollution Control