- FMA
- The Fabricator
- FABTECH
- Canadian Metalworking
Our Publications
Categories
- Additive Manufacturing
- Aluminum Welding
- Arc Welding
- Assembly and Joining
- Automation and Robotics
- Bending and Forming
- Consumables
- Cutting and Weld Prep
- Electric Vehicles
- En Español
- Finishing
- Hydroforming
- Laser Cutting
- Laser Welding
- Machining
- Manufacturing Software
- Materials Handling
- Metals/Materials
- Oxyfuel Cutting
- Plasma Cutting
- Power Tools
- Punching and Other Holemaking
- Roll Forming
- Safety
- Sawing
- Shearing
- Shop Management
- Testing and Measuring
- Tube and Pipe Fabrication
- Tube and Pipe Production
- Waterjet Cutting
Industry Directory
Webcasts
Podcasts
FAB 40
Advertise
Subscribe
Account Login
Search
Sciaky's EBAM process achieves qualification for huge satellite fuel tanks
- July 19, 2018
- News Release
- Additive Manufacturing
Chicago-based Sciaky Inc., a subsidiary of Phillips Service Industries Inc. (PSI) and a provider of metal additive manufacturing (AM) technology, has achieved qualification with its Electron Beam Additive Manufacturing (EBAM®) process, stemming from the completion of qualification testing performed by Lockheed Martin Space on a multiyear development program to create giant, high-pressure tanks that carry fuel for satellites.
Including the middle tank, the titanium vessel is about 8 ft. tall. Lockheed Martin, which 3-D-printed both halves of the 46-in. titanium fuel tank domes on an EBAM 110 machine, said the tanks met or exceeded the performance and reliability required by NASA, allowing them to become a standard product option on LM 2100 satellites.
Related Companies
- Podcasting
- Podcast:
- The Fabricator Podcast
- Published:
- 05/14/2024
- Running Time:
- 62:12
Cameron Adams of Laser Precision, a contract metal fabricator in the Chicago area, joins the podcast to talk...
- Trending Articles
- Industry Events
Laser Welding Certificate Course
- May 7 - August 6, 2024
- Farmington Hills, IL
World-Class Roll Forming Workshop
- June 5 - 6, 2024
- Louisville, KY
Advanced Laser Application Workshop
- June 25 - 27, 2024
- Novi, MI
Precision Press Brake Certificate Course
- July 31 - August 1, 2024
- Elgin,