- FMA
- The Fabricator
- FABTECH
- Canadian Metalworking
Categories
- Additive Manufacturing
- Aluminum Welding
- Arc Welding
- Assembly and Joining
- Automation and Robotics
- Bending and Forming
- Consumables
- Cutting and Weld Prep
- Electric Vehicles
- En Español
- Finishing
- Hydroforming
- Laser Cutting
- Laser Welding
- Machining
- Manufacturing Software
- Materials Handling
- Metals/Materials
- Oxyfuel Cutting
- Plasma Cutting
- Power Tools
- Punching and Other Holemaking
- Roll Forming
- Safety
- Sawing
- Shearing
- Shop Management
- Testing and Measuring
- Tube and Pipe Fabrication
- Tube and Pipe Production
- Waterjet Cutting
Industry Directory
Webcasts
Podcasts
FAB 40
Advertise
Subscribe
Account Login
Search
Trailer manufacturer replaces conventional steel HSS tube frame components with HSLA, reduces weight, increases durability
Substitute material is lighter, stronger, harder than conventional steel
- April 12, 2018
- Article
- Tube and Pipe Fabrication
Situation
XL Specialized Trailers, Manchester, Iowa, sought a way to reduce the weight of one of its products, a bottom-dump trailer. A manufacturer of heavy-haul trailers for commercial, construction, agricultural, wind energy, oil and gas, and custom transportation applications, the company has a competitive interest in weight reduction. Reducing a trailer’s weight is a productivity enhancement, providing the opportunity to carry larger, heavier loads within the legal load limit.
After XL was purchased by Bull Moose Tube in 2016, it had a partner with a vested interest in improving its products. Bull Moose Tube has a niche in tube production, using a high-strength, low-alloy (HSLA) steel and forming square and rectangular hollow structural sections directly from strip. By forming the shape directly rather than forming it round as an intermediate step, the process minimizes cold-working, which changes steel’s characteristics. Through this process, Bull Moose has created Stratusteel®, an HSLA that is about 2.5 times stronger and three times harder than conventional steel tubing.
In 2016, the two companies pursued a proof of concept, whereby the proprietary alloy would be used for the frame of the company’s 60 BD bottom-dump trailer.
Resolution
While the XL team worked on new designs, Bull Moose Tube’s engineering team provided input and advice in three areas. First was finite element analysis, providing computer-aided structural design optimization and checks on stresses and loads related to various design concepts. Second was welding. Bull Moose provided a thermal analysis with instructions for keeping the weld temperatures down to prevent altering the steel’s characteristics. The Bull Moose team also weighed in regarding a testing regimen.
For the initial proof of concept, XL and Bull Moose opted not to alter the current XL 60 BD design, but rather to simply replace the steel. All other design elements were kept constant.
The proprietary alloy allows XL to use far less material. The substitution removed 1,100 pounds from the 5,500-lb. frame, for a 20 percent reduction in the frame weight. The total (unloaded) weight of the trailer was reduced from 12,900 lbs. to 11,800 lbs. Given an 80,000-lb. legal load limit for over-the-road use, this new trailer allows operators to haul 1,100 lbs. more per trip, equivalent to one free haul for every 50 fully loaded hauls.
Another benefit is the material’s hardness, which increases its impact resistance, keeping it looking newer longer.
Through a distribution partner, Midco Sales LLC, XL identified an enduser, Arizona-based Gila River Sand & Gravel, that was eager to use the new trailer. The test trailer operated out of Gila River’s Maricopa plant, hauling eight to 12 loads of rock and concrete sand to and from a concrete producer over more than a half mile of dirt and more than 10 miles of highway each way. In addition, Gila River took the trailer to construction sites, hauling aggregate base course material on road projects.
Driver reports on the trailer were good regarding tracking and ride. Most notably, the owner found no evidence of wear in the frame, the fifth-wheel pin or plate, brakes, or air systems, which are areas of concern for Gila River.
The weight savings balanced well with the investment cost. Getting one free load for every 50 loads resulted in a three-year return on investment (ROI) for Gila River Sand & Gravel. The test trailer is expected to be robust and durable enough to yield an overall life span of seven to 10 years, well beyond the three-year ROI period.
Bull Moose Tube Co., 1819 Clarkson Road, Chesterfield, MO 63017, 636-537-2600, www.bullmoosetube.com
About the Publication
Related Companies
subscribe now
The Tube and Pipe Journal became the first magazine dedicated to serving the metal tube and pipe industry in 1990. Today, it remains the only North American publication devoted to this industry, and it has become the most trusted source of information for tube and pipe professionals.
start your free subscription- Stay connected from anywhere
Easily access valuable industry resources now with full access to the digital edition of The Fabricator.
Easily access valuable industry resources now with full access to the digital edition of The Welder.
Easily access valuable industry resources now with full access to the digital edition of The Tube and Pipe Journal.
Easily access valuable industry resources now with full access to the digital edition of The Fabricator en Español.
- Podcasting
- Podcast:
- The Fabricator Podcast
- Published:
- 05/14/2024
- Running Time:
- 62:12
Cameron Adams of Laser Precision, a contract metal fabricator in the Chicago area, joins the podcast to talk...
- Trending Articles
Making the move from hard automation to robotic welding
Students learn fabrication one piece at a time
Miscellaneous metals fabricator increases productivity and opportunity with plasma cutting
Get a grip on the misunderstood tube bender motor starter
Manufacturing finally sees some sunshine
- Industry Events
Laser Welding Certificate Course
- May 7 - August 6, 2024
- Farmington Hills, IL
World-Class Roll Forming Workshop
- June 5 - 6, 2024
- Louisville, KY
Advanced Laser Application Workshop
- June 25 - 27, 2024
- Novi, MI
Precision Press Brake Certificate Course
- July 31 - August 1, 2024
- Elgin,