TPJ - The Tube & Pipe Journal®

Cutting to the chase

Assessing cutting methods' suitability for inline end forming, bending

By William Holyoak
January 10, 2006

Many tube cut-off machines have evolved to integrate end forming and bending capabilities that normally are considered secondary operations. The suitability of a cutting method to be integrated in-line with end forming and bending depends on each cutting method’s characteristics and the bending and end forming requirements. The best prospects are the rotary cut and the laser, because they produce minimal chips and burrs and provide an end condition suitable for inline end forming, and bending.

Tube cutoff machines have evolved to integrate end forming and bending capabilities that normally are considered secondary operations. Inline operations are most applicable to long runs and dedicated applications. They have limited practicability for short-run work that requires a lot of tooling changeover.

Many tube cutoff machines have evolved to integrate end forming and bending capabilities that normally are considered secondary operations. Considering the tube industry's need to reduce costs to stay competitive, the concept of integrating more operations may sound appealing. An inline system offers the following benefits:

  • Reduced labor by combining operations into a single machine
  • Improved quality control
  • Reduced floor space requirements
  • Improved inventory control
  • Less capital investment

It is not, however, a panacea. A cutting method's suitability for an integrated cutoff machine that performs cutting, end forming, and bending inline depends on the cutting method's characteristics and the bending and end forming requirements.

Burrs. In mandrel bending, the tube end at the cut must have a minimum ID intrusion so as not to affect the mandrel operation. Since an inline system usually does not have a postfinishing operation, the cut made by the inline machine must be clean and burr-free.

Cut Quality. Similarly, cut quality can affect the results of end forming, because material is displaced to provide the final shape. Variations in material volume can affect the final tolerances, particularly if the tube is to receive a complex or aggressive end form. In addition, many cutting methods can potentially change the hardness of the tube in the immediate area of the cut. Work hardening, or even annealing, of the material can have a negative impact on the end form process, so it is important that the cut process has a minimal impact on the tube end.

Tube Cutting Systems

The main tube cutting methods are:

  • Cold saw
  • Abrasive wheel
  • Band saw
  • Lathe
  • Plasma
  • Shear
  • Rotary
  • Laser

Each of these cutting methods has specific capabilities and limitations that make it suitable for certain applications (see Figure 1).

Tube Cutting Characteristics and Inline Forming Applicability
Cutoff Method
Advantages Limitations Inline Adaptability Comments
Cold Saw
• Fast
• Inexpensive
• Cuts odd shapes

• Chips
• Material loss

Very limited Suitable for a fast,
inexpensive cut where
chips and material loss
are not critical
Abrasive Wheel • High cut speed
• Cuts odd shapes
• Abrasive dust
• Material loss
Very limited Similar to saw cut, but with improved cut speed
Band Saw

• Cuts larger-diameter tube/pipe • Chips
• Material loss
• Limited for automation
Not practical Not very practical for automation
Nick and Shear


• Fast
• Excellent on hard materials
• Burrs
• Not good for soft materials
• Material loss
Limited Automation better suited for transfer line
Lathe Cut

• Cuts desired
end and OD/ID shapes
• High cut quality
• Chips
• Lubricant/coolant is required
• Material loss
Limited Automation is limited to transfer line applications with integrated cleaning
Rotary Cut




• Chipless
• End condition good for all but the most complicated end forms
• Complicated end forms (4+ hits) require end finish
• Not applicable for heavy-wall tube
(> 0.100')
Good Best cutting method for integrated, inline systems
Laser





• Chipless
• Cuts exotic
materials
• Can cut precise shapes
• Relatively expensive
• Material loss
• May require end finishing prior to
end forming
Good
Limited
Suitable for applications requiring high cut quality, such as for mandrel bending, and reduced secondary operations
Figure 1

Saw, Abrasive Wheel, Lathe, Shear, Plasma Cutter. If the end condition is not critical, a cold saw or band saw is the fastest and least expensive cutting method. While saws are widely used, their ability to integrate secondary functions is limited because this cutting process creates chips, which requires a cleaning operation as part of the process. The same is true for abrasive wheel and lathe cutting. Plasma cutting often produces slag and burrs, which must be removed before end forming. A shear cutter creates a burr as it wipes some of the material beyond the tube wall cross section, especially on hard materials. Although if the process to be integrated is ram bending—the process typically used in wire forming systems—the end condition is not critical.

Each of these cutting methods creates contaminating conditions such as chips, dust, and burrs that interfere with the secondary inline operation and leave an end condition unsuitable for a single integrated machine to achieve multiple operations. They require a workcell or additional finishing and cleaning stations in which cleaning and burr removal can be performed inline with the cutting process.

The presence of burrs in bending or end form tooling either interferes with the ability to insert the mandrel in bending or with the basic loading of the tube in an automatic machine. In end forming, burrs on either the ID or OD of a tube become packed into voids in the tool form, affecting the tool's ability to maintain tolerances or generate the final shape.

Rotary Cutting, Laser Cutting. Although most cutting methods can be integrated into an automatic system, very few are applicable for an inline system. The best prospects are the rotary cutter and the laser, because they produce minimal chips and burrs and produce an end condition suitable for inline end forming and bending (see Figure 2).

Figure 2
Because rotary tube cutting produces minimal chipping and burrs, it leaves an end condition suitable for inline end forming and bending of most tube types. It is not applicable for tube walls thicker than 0.1 inch.

The rotary cutter has been used in inline as well as stand-alone end forming machines for several decades. The rotary cut displaces material through the use of an angled, rotating cutter wheel, creating a clean, chipless cut. When minimal ID intrusion of the tube is critical, a pull-apart system is added to pull the tube apart after approximately 90 percent of the tube wall has been penetrated.

Because the cutter wheel penetrates the tube at an angle, the end condition has a slight taper reflecting the cutter shape. However, since the process is accurate, produces minimal work hardening, and is chipless, the taper effect on all but the most aggressive end forming is minimal. It achieves the desired fill ratio to form a good part for approximately 80 percent of the parts used by industry.

Usually shapes that require four or more hits to achieve the desired shape require a tube end that is postprocessed or laser-cut. A laser provides good cut quality, minimal distortion, and minimal material loss in the kerf.

Lasers have been integrated into inline systems. However, they are a relatively expensive capital equipment expenditure compared with conventional cutoff equipment and have had limited use for continuous tube cutoff applications for this reason. They are generally considered justifiable for applications that require high cut quality and a reduction of secondary operations.

Inline lasers are suitable for generating unusual or complex shapes at the tube end. Because their clean cut creates minimal distortion, they are highly suitable for mandrel tube bending.

However, work hardening of the tube end from the thermal effect of the cutting process may reduce lasers' practicality for use in end forming operations, particularly the most difficult ones.

Tube Forming Systems

Some of the forming operations that can be integrated inline are:

  • Double end chamfering (end finishing) of tubing without cut length limitations, for automotive and aircraft brake, fuel, and hydraulic line applications

  • Punch end forming, makes up to four sequential hits to form beads, flares, bell ends, and more complex automotive and aircraft shapes that can be accomplished within the four-hit limit

  • CNC bending and end finishing used in the air conditioning and automotive industries for simple bends not requiring a mandrel and end-formed subassemblies

  • Spin end forming, which uses rotating friction dies to form a closed end on copper tubes (see Figure 3) such as tube end closing, reduction, or expansion
Figure 3
These thermocouple components were produced in 1.2 seconds per part in an inline tube cutoff machine. Tubes were cut-to-length and end-formd with a closed end and precision center hole.

Inline operations are most suitable for long runs and dedicated applications. They have limited practicability for short-run work that requires a lot of tooling changeover. When bending is incorporated into the system, the use of mandrels is not practical. The use of inline systems also should be limited to proven, durable forming technologies to ensure that the overall operating efficiency of the system is high enough to provide the anticipated payback.

Looking Ahead

The next advances in tube processing integration are likely to involve some forms of simple assembly so that a complete subassembly can be produced from coil to finished product. In certain applications, this will be very cost-effective. It is unlikely that complex assembly operations will be integrated, however—they probably will continue to be done in an integrated workcell.

William Holyoak is past president, T-Drill Industries Inc., 1740 Corporate Drive, No. 820, Norcross, GA 30093, 770-925-0520, fax 770-925-3912, b2holy@tds.net, www.t-drill.com. He also is the recipient of the 2005 TPA Outstanding Contribution Award.


TAGS: end finishing, t-drill industries inc., tube and pipe, tube bending, tube end forming, william holyoak




How Do you Rate This Article?            
Poor 5  Great

Comments:

Email address (optional):

Want more information?

Learn more about this company:

Tube and pipe production technical articles


 
  • Sponsors
  • Thermatool Corp.
  • Tube Dusseldorf 2010 - Techcell Banner
  • Tube India - Techcell Banner
Fabricators and Manufacturers Association, International Tube and Pipe Association, International