Core products CE-approved for sale in Europe

June 16, 2009

Core products CE-approved for sale in Europe

Fischer Engineering Co., Dayton, Ohio, has announced that its core products— weld bend testers, weld tensile testers, and welding coupons— have been CE-approved for sale in Europe.

For more information, visit the Fischer Engineering Co. showroom.