Model or Series Electron Beam ERW High frequency Contact ERW High frequency Induction ERW Rotary Wheel Direct Current DC ERW Rotary Wheel Square Wave Laser Plasma Spiral Welding TIG GTAW OD Minimum Inches OD Maximum Inches Wall Thickness Minimum Inches Wall Thickness Maximum Inches Mild Steel Stainless Steel Aluminum Copper Other Metals Round Square Rectangle Other Shapes

 T & H LEMONT INC. Countryside, IL   Hot Link

WU-8           checkbox     checkbox .090 .375 .006 .035 checkbox checkbox checkbox checkbox checkbox checkbox      
WU-11     checkbox checkbox   checkbox     checkbox .150 .750 .010 .050 checkbox checkbox checkbox checkbox checkbox checkbox checkbox checkbox checkbox
WU-11M     checkbox checkbox   checkbox     checkbox .250 1.000 .020 .065 checkbox checkbox checkbox checkbox checkbox checkbox checkbox checkbox checkbox
WU-15     checkbox checkbox   checkbox     checkbox .375 1.750 .020 .083 checkbox checkbox checkbox checkbox checkbox checkbox checkbox checkbox checkbox
WU-20     checkbox checkbox   checkbox     checkbox .500 2.500 .020 .134 checkbox checkbox checkbox checkbox checkbox checkbox checkbox checkbox checkbox
WU-25     checkbox checkbox   checkbox checkbox   checkbox .750 3.500 .025 .160 checkbox checkbox checkbox checkbox checkbox checkbox checkbox checkbox checkbox
WU-35     checkbox checkbox   checkbox checkbox   checkbox 1.000 4.500 .060 .240 checkbox checkbox checkbox checkbox checkbox checkbox checkbox checkbox checkbox
WU-40     checkbox checkbox   checkbox checkbox   checkbox 1.500 5.500 .060 .280 checkbox checkbox checkbox checkbox checkbox checkbox checkbox checkbox checkbox
WU-50     checkbox checkbox   checkbox checkbox   checkbox 2.000 6.625 .080 .330 checkbox checkbox checkbox checkbox checkbox checkbox checkbox checkbox checkbox
WU-60     checkbox checkbox   checkbox checkbox   checkbox 2.000 8.625 .110 .375 checkbox checkbox checkbox checkbox checkbox checkbox checkbox checkbox checkbox

 ABBEY INTERNATIONAL LTD. Perrysburg, OH

1K - 1.5     checkbox     checkbox     checkbox .375 1.500 .018 .083 checkbox checkbox     checkbox checkbox checkbox   checkbox
2X - 2.25     checkbox     checkbox     checkbox .500 2.250 .020 .095 checkbox checkbox     checkbox checkbox checkbox checkbox checkbox
2K - 3.5     checkbox     checkbox     checkbox .625 3.687 .028 .125 checkbox checkbox     checkbox checkbox checkbox checkbox checkbox
3X - 3.5     checkbox     checkbox     checkbox .750 3.500 .032 .160 checkbox checkbox     checkbox checkbox checkbox checkbox checkbox
3K - 3.5     checkbox           checkbox .840 3.500 .042 .203 checkbox checkbox     checkbox checkbox checkbox checkbox checkbox
4X - 5.0     checkbox     checkbox     checkbox 1.250 5.000 .042 .188 checkbox checkbox     checkbox checkbox checkbox checkbox checkbox
4K - 4.5     checkbox           checkbox 1.000 4.500 .049 .250 checkbox checkbox     checkbox checkbox checkbox checkbox checkbox
5K - 5.625     checkbox             1.250 5.625 .049 .250 checkbox         checkbox checkbox checkbox checkbox
6X - 6.625     checkbox     checkbox     checkbox 1.900 6.625 .049 .237 checkbox checkbox       checkbox checkbox checkbox checkbox
6K - 6.625     checkbox             1.900 6.625 .083 .338 checkbox         checkbox checkbox checkbox checkbox
7X - 7.5     checkbox             2.375 7.500 .065 .280 checkbox         checkbox checkbox checkbox checkbox
7K - 7.5     checkbox             2.375 7.500 .083 .340 checkbox         checkbox checkbox checkbox checkbox
8K - 8.75   checkbox checkbox             2.875 8.750 .083 .375 checkbox         checkbox checkbox checkbox checkbox
12X - 12.75   checkbox checkbox             3.500 12.750 .083 .330 checkbox         checkbox checkbox checkbox checkbox
12K - 12.75   checkbox checkbox             3.500 12.750 .120 .625 checkbox         checkbox checkbox checkbox  
16K - 16.0   checkbox checkbox             4.500 16.000 .120 .625 checkbox         checkbox checkbox checkbox  
20K - 20.00   checkbox checkbox             6.625 20.000 .120 .500 checkbox         checkbox checkbox checkbox  
24K - 24.00   checkbox checkbox             8.625 24.000 .188 .750 checkbox         checkbox checkbox checkbox  
27K - 27.00   checkbox checkbox             10.750 27.000 .200 .750 checkbox         checkbox checkbox checkbox  
36K - 30.0   checkbox checkbox             14.000 36.000 .188 1.000 checkbox         checkbox checkbox checkbox  

 ABC METAL CO. Rockford, IL

wsresdf checkbox   checkbox   checkbox   checkbox     0.34 0.34 0.34 0.34 checkbox   checkbox   checkbox   checkbox   checkbox

 ADDISON MACHINE ENGINEERING INC. Reedsburg, WI

AM-050           checkbox checkbox   checkbox .125 .500 .005 .030 checkbox checkbox checkbox checkbox checkbox checkbox checkbox checkbox checkbox
AM-075           checkbox checkbox   checkbox .188 .750 .007 .035 checkbox checkbox checkbox checkbox checkbox checkbox checkbox checkbox checkbox
AM-1000   checkbox checkbox checkbox checkbox checkbox checkbox   checkbox .250 1.000 .010 .049 checkbox checkbox checkbox checkbox checkbox checkbox checkbox checkbox checkbox
AM-1500   checkbox checkbox checkbox checkbox checkbox checkbox   checkbox .250 1.500 .015 .065 checkbox checkbox checkbox checkbox checkbox checkbox checkbox checkbox checkbox
AM-1500X   checkbox checkbox checkbox checkbox checkbox checkbox   checkbox .375 1.750 .020 .083 checkbox checkbox checkbox checkbox checkbox checkbox checkbox checkbox checkbox
AM-2000   checkbox checkbox checkbox checkbox checkbox checkbox   checkbox .500 2.250 .025 .125 checkbox checkbox checkbox checkbox checkbox checkbox checkbox checkbox checkbox
AM-2500   checkbox checkbox checkbox checkbox checkbox checkbox   checkbox .750 3.000 .030 .160 checkbox checkbox checkbox checkbox checkbox checkbox checkbox checkbox checkbox
AM-3000   checkbox checkbox checkbox checkbox   checkbox   checkbox 1.000 4.000 .040 .200 checkbox checkbox checkbox checkbox checkbox checkbox checkbox checkbox checkbox
AM-4000   checkbox checkbox checkbox checkbox checkbox checkbox   checkbox 1.250 5.000 .050 .250 checkbox checkbox checkbox checkbox checkbox checkbox checkbox checkbox checkbox
AM-4500   checkbox checkbox checkbox checkbox checkbox checkbox   checkbox 1.500 5.500 .060 .300 checkbox checkbox checkbox checkbox checkbox checkbox checkbox checkbox checkbox
AM-5000   checkbox checkbox checkbox checkbox checkbox checkbox   checkbox 1.750 6.000 .075 .335 checkbox checkbox checkbox checkbox checkbox checkbox checkbox checkbox checkbox
AM-6000   checkbox checkbox checkbox checkbox checkbox checkbox   checkbox 2.000 7.625 .090 .375 checkbox checkbox checkbox checkbox checkbox checkbox checkbox checkbox checkbox

 CROWN HOLLANDER MACHINERY INC. Toronto, ON Canada

CM2000/25               checkbox   16.0 118.0 0.250 1.0 checkbox checkbox checkbox     checkbox      
ELBM   checkbox             checkbox 0.500 8.0 0.1 0.500 checkbox checkbox       checkbox checkbox checkbox  

 DREISTERN INC. Telford, PA

RS 060   checkbox checkbox checkbox checkbox checkbox checkbox   checkbox .100 1.000 .006 .040 checkbox checkbox checkbox checkbox checkbox checkbox checkbox checkbox checkbox
RS 080   checkbox checkbox checkbox checkbox checkbox checkbox   checkbox .125 1.500 .010 .040 checkbox checkbox checkbox checkbox checkbox checkbox checkbox checkbox checkbox
RS 100   checkbox checkbox checkbox checkbox checkbox checkbox   checkbox .400 2.000 .016 .063 checkbox checkbox checkbox checkbox checkbox checkbox checkbox checkbox checkbox
RS 125   checkbox checkbox checkbox checkbox checkbox checkbox   checkbox .500 3.000 .020 .120 checkbox checkbox   checkbox checkbox checkbox checkbox checkbox checkbox
RS 160   checkbox checkbox checkbox checkbox checkbox checkbox   checkbox .700 4.000 .024 .160 checkbox checkbox checkbox checkbox checkbox checkbox checkbox checkbox checkbox
RS 200   checkbox checkbox checkbox checkbox checkbox checkbox   checkbox .500 6.000 .030 .200 checkbox checkbox checkbox checkbox checkbox checkbox checkbox checkbox checkbox
RS 250   checkbox checkbox checkbox checkbox checkbox checkbox   checkbox .500 8.000 .040 .275 checkbox checkbox checkbox checkbox checkbox checkbox checkbox checkbox checkbox
RSD 50-1           checkbox checkbox   checkbox .250 1.000 .006 .010 checkbox checkbox checkbox checkbox checkbox checkbox checkbox checkbox checkbox
RSD 50-2           checkbox checkbox   checkbox .750 2.000 .008 .016 checkbox checkbox checkbox checkbox checkbox checkbox checkbox checkbox  

 IPG PHOTONICS CORP. Oxford, MA

Fiber Lasers           checkbox                                

 KIPCO INTL. INC. Auburndale, FL

KE-1T                 checkbox .240 .625 .012 .040   checkbox checkbox checkbox checkbox checkbox checkbox checkbox  
KE-2T                 checkbox .374 1.500 .016 .059   checkbox checkbox checkbox checkbox checkbox checkbox checkbox  
KE-3T                 checkbox .636 2.000 .024 .098   checkbox checkbox checkbox checkbox checkbox checkbox checkbox  
KE-4T                 checkbox 1.000 3.000 .031 .157   checkbox checkbox checkbox checkbox checkbox checkbox checkbox  
KE-5T             checkbox   checkbox 1.250 4.000 .047 .197   checkbox checkbox checkbox checkbox checkbox checkbox checkbox  
KE-6T             checkbox   checkbox 2.000 6.614 .059 .236   checkbox checkbox checkbox checkbox checkbox checkbox checkbox  
KE-7T             checkbox   checkbox 8.500 12.75 .071 .295   checkbox checkbox checkbox checkbox checkbox checkbox checkbox  
KE -16 c             checkbox   checkbox 6 16 .080 .250   checkbox       checkbox      
KE-24-cfg TPT             checkbox     10 24 .125 .400   checkbox checkbox checkbox   checkbox      

 METALS INTERNATIONAL LTD. Shanghai, China

    checkbox checkbox         checkbox   1/2 120 0.06 2 checkbox checkbox       checkbox checkbox checkbox  

 MILL MASTERS INC. Jackson, TN

Elite Series E-1234     checkbox             .475 1.35 .010 .025 checkbox checkbox checkbox checkbox         checkbox
Elite Series E-1485     checkbox             .551 Flat Oval 3.34 Flat Oval .012 .040 checkbox checkbox checkbox checkbox checkbox       checkbox
Spectrum Series S-626     checkbox             .236 1.024 .010 .040 checkbox   checkbox checkbox checkbox checkbox checkbox checkbox checkbox
Spectrum Series S-1976     checkbox             .748 2.992 .015 .118 checkbox   checkbox checkbox checkbox checkbox checkbox checkbox checkbox
Premier Series P-626T           checkbox     checkbox .236 1.024 .010 .039 checkbox checkbox checkbox checkbox checkbox checkbox checkbox checkbox checkbox
Premier Series P-1976T           checkbox     checkbox .748 4.50 .015 .118 checkbox checkbox checkbox checkbox checkbox checkbox checkbox checkbox checkbox
Ultra Tube Mill     checkbox             .197 1.024 .009 .039 checkbox   checkbox checkbox checkbox checkbox     checkbox

 MYUNG JIN MACHINERY CO. LTD. Siheung-City, Gyeonggi-Do South Korea

MJM-TM010-L     checkbox             .314 1.000 .027 .078 checkbox checkbox       checkbox checkbox checkbox checkbox
MJM-TM015-L     checkbox             .500 1.500 .027 .094 checkbox checkbox       checkbox checkbox checkbox checkbox
MJM-TM020-L     checkbox             .681 2.000 .031 .125 checkbox checkbox       checkbox checkbox checkbox checkbox
MJM-TM025-L     checkbox             .854 2.381 .031 .141 checkbox checkbox       checkbox checkbox checkbox checkbox
MJM-TM030-L     checkbox             1.000 3.003 .039 .177 checkbox checkbox       checkbox checkbox checkbox checkbox
MJM-TM040-L     checkbox             1.338 3.507 .039 .177 checkbox checkbox       checkbox checkbox checkbox checkbox
MJM-TM050-L     checkbox             1.338 4.500 .062 .196 checkbox checkbox       checkbox checkbox checkbox checkbox
MJM-TM060-L     checkbox             2.381 6.625 .078 .255 checkbox checkbox       checkbox checkbox checkbox checkbox
MJM-TM080-L     checkbox             3.507 8.625 .125 .314 checkbox checkbox       checkbox checkbox checkbox checkbox
MJM-TM120-L     checkbox             4.500 12.751 .188 .421 checkbox checkbox       checkbox checkbox checkbox checkbox
MJM-TM160-L   checkbox checkbox             6.625 16.000 .188 .629 checkbox checkbox       checkbox checkbox checkbox checkbox
MJM-TM200-L   checkbox checkbox             6.625 20.000 .220 .708 checkbox checkbox       checkbox checkbox checkbox checkbox
MJM-TM240-L   checkbox checkbox             8.625 24.015 .236 .787 checkbox checkbox       checkbox checkbox checkbox checkbox

 NIRMAL MANUFACTURING & ALLIED INDUSTRIES LTD. New Delhi, India

N-TM   checkbox checkbox checkbox checkbox checkbox checkbox   checkbox 0.5 24 0.01 0.70 checkbox checkbox     checkbox checkbox checkbox checkbox checkbox

 OFFICINE MTM S.P.A. Spinea (Venezia), Italy

MTM 40 C     checkbox     checkbox checkbox   checkbox .394 .984 .012 .048 checkbox checkbox checkbox checkbox checkbox checkbox checkbox checkbox checkbox
MTM 50 C     checkbox     checkbox checkbox   checkbox .394 1.975 .020 .098 checkbox checkbox checkbox checkbox checkbox checkbox checkbox checkbox checkbox
MTM 60 C     checkbox     checkbox checkbox   checkbox .472 2.480 .028 .118 checkbox checkbox checkbox checkbox checkbox checkbox checkbox checkbox checkbox
MTM 70 C     checkbox     checkbox checkbox   checkbox .630 3.000 .035 .157 checkbox checkbox checkbox checkbox checkbox checkbox checkbox checkbox checkbox
MTM 80 C     checkbox     checkbox checkbox   checkbox .827 3.150 .039 .177 checkbox checkbox checkbox checkbox checkbox checkbox checkbox checkbox checkbox
MTM 90 C     checkbox     checkbox checkbox   checkbox .984 3.500 .039 .197 checkbox checkbox checkbox checkbox checkbox checkbox checkbox checkbox checkbox
MTM 100 C     checkbox     checkbox checkbox   checkbox 1.300 4.480 .039 .217 checkbox checkbox checkbox checkbox checkbox checkbox checkbox checkbox checkbox
MTM 120 C     checkbox     checkbox checkbox   checkbox 1.655 5.000 .059 .236 checkbox checkbox checkbox checkbox checkbox checkbox checkbox checkbox checkbox
MTM 130 C     checkbox     checkbox checkbox   checkbox 2.480 6.625 .059 .280 checkbox checkbox checkbox checkbox checkbox checkbox checkbox checkbox checkbox
MTM 160 C     checkbox     checkbox checkbox   checkbox 3.500 8.625 .079 .315 checkbox checkbox checkbox checkbox checkbox checkbox checkbox checkbox checkbox

 OTO MILLS S.P.A St. Charles, IL

OTO 201           checkbox     checkbox .314 .787 .016 .06 checkbox checkbox checkbox checkbox checkbox checkbox      
OTO 322     checkbox checkbox checkbox checkbox     checkbox .374 1.259 .024 .1 checkbox checkbox checkbox checkbox checkbox checkbox checkbox checkbox checkbox
OTO 503     checkbox checkbox checkbox checkbox     checkbox .5 2 .024 .12 checkbox checkbox checkbox checkbox checkbox checkbox checkbox checkbox checkbox
OTO 763     checkbox checkbox checkbox checkbox     checkbox .629 3 .024 .12 checkbox checkbox checkbox checkbox checkbox checkbox checkbox checkbox checkbox
OTO 764     checkbox checkbox checkbox checkbox checkbox   checkbox .75 3 .032 .16 checkbox checkbox checkbox checkbox checkbox checkbox checkbox checkbox checkbox
OTO 895   checkbox checkbox checkbox checkbox checkbox checkbox   checkbox .825 3.5 .048 .22 checkbox checkbox checkbox checkbox checkbox checkbox checkbox checkbox checkbox
OTO 1274     checkbox     checkbox checkbox     2.500 5.000 .100 .160 checkbox checkbox     checkbox checkbox checkbox checkbox checkbox
OTO 1276   checkbox checkbox     checkbox checkbox     2.500 5.000 .100 ,240 checkbox checkbox     checkbox checkbox checkbox checkbox checkbox
OTO 1687   checkbox checkbox     checkbox checkbox     3.000 6.625 .125 .280 checkbox checkbox     checkbox checkbox checkbox checkbox checkbox
OTO 16812   checkbox checkbox     checkbox checkbox     3.500 6.625 .187 .500 checkbox checkbox     checkbox checkbox checkbox checkbox checkbox
OTO 21912   checkbox checkbox     checkbox checkbox     5.000 8.625 .187 .500 checkbox checkbox     checkbox checkbox checkbox checkbox checkbox

 PLASMA TEAM S.N.C. Arquata Scrivia, Italy

PAW Series 5000             checkbox     2 10 .100 .600 checkbox checkbox       checkbox      

 RAFTER EQUIPMENT CORP. Strongsville, OH

RT-1000     checkbox     checkbox     checkbox 0.250 1.000 0.010 0.049 checkbox checkbox       checkbox checkbox checkbox checkbox
RT-1250     checkbox     checkbox     checkbox 0.250 1.250 0.020 0.065 checkbox checkbox       checkbox checkbox checkbox checkbox
RT-1500     checkbox     checkbox     checkbox 0.375 1.750 0.020 0.083 checkbox checkbox checkbox     checkbox checkbox checkbox checkbox
RT-2000S     checkbox     checkbox     checkbox 0.500 3.000 0.028 0.135 checkbox checkbox checkbox     checkbox checkbox checkbox checkbox
RT-2500     checkbox     checkbox     checkbox 0.075 3.000 0.032 0.165 checkbox checkbox checkbox     checkbox checkbox checkbox checkbox
RT-3000     checkbox     checkbox     checkbox 0.750 4.000 0.032 0.188 checkbox checkbox checkbox     checkbox checkbox checkbox checkbox
RT-3500     checkbox     checkbox     checkbox 1.000 5.000 0.048 0.250 checkbox checkbox       checkbox checkbox checkbox checkbox
RT-4500     checkbox     checkbox     checkbox 1.250 6.000 0.060 0.300 checkbox checkbox       checkbox checkbox checkbox checkbox
RT-6000   checkbox checkbox     checkbox     checkbox 2.500 8.625 0.065 0.440 checkbox checkbox       checkbox checkbox checkbox checkbox
RT-8000   checkbox checkbox             4.000 12.750 0.065 0.500 checkbox checkbox       checkbox checkbox checkbox checkbox
RT-9000   checkbox checkbox             6.625 16.000 0.120 0.625 checkbox checkbox       checkbox checkbox checkbox checkbox

 ROLLFORM EQUIPMENT PVT. LTD. Distt Ghaziabad, U.P. India

PTM-L-25     checkbox     checkbox     checkbox 0.314 1.000 0.0119 0.0394 checkbox checkbox       checkbox checkbox checkbox checkbox
PTM-L-32     checkbox     checkbox     checkbox 0.374 1.25 0.0119 0.063 checkbox checkbox       checkbox checkbox checkbox checkbox
PTM-H-38     checkbox     checkbox     checkbox 0.374 1.5 0.158 0.0985 checkbox checkbox       checkbox checkbox checkbox checkbox
PTM-H-38     checkbox     checkbox     checkbox 0.374 1.5 0.158 0.0985 checkbox checkbox       checkbox checkbox checkbox checkbox
PTM-H-50     checkbox     checkbox     checkbox 0.50 2.0 0.158 0.0985 checkbox checkbox       checkbox checkbox checkbox checkbox
PTM-H-76   checkbox checkbox     checkbox     checkbox 0.625 2.5 0.0237 0.177 checkbox checkbox       checkbox checkbox checkbox checkbox
PTM-H-81   checkbox checkbox     checkbox     checkbox 0.625 3.2 0.0237 0.191 checkbox checkbox       checkbox checkbox checkbox checkbox
PTM-H-100   checkbox checkbox     checkbox     checkbox 1.00 4.00 0.0394 0.2126 checkbox checkbox       checkbox checkbox checkbox checkbox
PTM-H-127   checkbox checkbox     checkbox     checkbox 1.5 5.00 0.0437 0.2126 checkbox checkbox       checkbox checkbox checkbox checkbox
TM-H-150   checkbox checkbox             2.381 6.625 0.78 0.255 checkbox         checkbox checkbox checkbox checkbox
TM-H-200   checkbox checkbox             3.507 8.625 0.125 0.314 checkbox         checkbox checkbox checkbox checkbox

 SOUTEC LTD Farmington Hills, MI

Soutube           checkbox       1.25 6 0.025 0.18 checkbox checkbox checkbox   checkbox checkbox checkbox checkbox checkbox
Soulex           checkbox checkbox     3 23.5 0.02 0.1 checkbox checkbox checkbox checkbox   checkbox checkbox   checkbox

 UNITHERM INDUCTOWELD (INDIA) PVT. LTD. Noida, U.P. India

PTM-L-25     checkbox     checkbox     checkbox .314 1.000 .0119 .0394 checkbox checkbox       checkbox checkbox checkbox checkbox
PTM-L-32     checkbox     checkbox     checkbox .374 1.25 .0119 .063 checkbox checkbox       checkbox checkbox checkbox checkbox
PTM-H-38     checkbox     checkbox     checkbox .374 1.5 .158 .0985 checkbox checkbox       checkbox checkbox checkbox checkbox
PTM-H-50     checkbox     checkbox     checkbox .50 2.0 .158 .0985 checkbox checkbox       checkbox checkbox checkbox checkbox
PTM-H-76   checkbox checkbox     checkbox     checkbox .625 2.5 .0237 .177 checkbox checkbox       checkbox checkbox checkbox checkbox
PTM-H-81   checkbox checkbox     checkbox     checkbox .625 3.2 .0237 .191 checkbox checkbox       checkbox checkbox checkbox checkbox
PTM-H-100   checkbox checkbox     checkbox     checkbox 1.00 4.00 .0394 .2126 checkbox checkbox       checkbox checkbox checkbox checkbox
PTM-H-127   checkbox checkbox     checkbox     checkbox 1.5 5.00 .0473 .2126 checkbox checkbox       checkbox checkbox checkbox checkbox
TM-H-150   checkbox checkbox             2.381 6.625 .78 .255 checkbox         checkbox checkbox checkbox checkbox
TM-H-200   checkbox checkbox             3.507 8.625 .125 .314 checkbox         checkbox checkbox checkbox checkbox

 YODER - A MEMBER OF THE FORMTEK GROUP Cleveland, OH

12" Pipe Mill   checkbox checkbox             4.500 12.750 .083 .625 checkbox checkbox checkbox checkbox checkbox checkbox checkbox checkbox checkbox
16" Pipe Mill   checkbox checkbox             4.500 16 .120 .625 checkbox checkbox checkbox checkbox checkbox checkbox checkbox checkbox checkbox
26" Pipe Mill   checkbox checkbox             6.625 28 .120 1.000 checkbox checkbox checkbox checkbox checkbox checkbox checkbox checkbox checkbox
6" Pipe Mill   checkbox checkbox             2.375 6.625 .065 .438 checkbox checkbox checkbox checkbox checkbox checkbox checkbox checkbox checkbox
8" Pipe Mill   checkbox checkbox             2.875 8.625 .083 .500 checkbox checkbox checkbox checkbox checkbox checkbox checkbox checkbox checkbox
M-1-1/2 & QVW-150   checkbox checkbox     checkbox     checkbox .313 1.250 .018 .049 checkbox checkbox checkbox checkbox checkbox checkbox checkbox checkbox checkbox
M-2 & QVW-200   checkbox checkbox     checkbox     checkbox .500 2.250 .018 .095 checkbox checkbox checkbox checkbox checkbox checkbox checkbox checkbox checkbox
M-2-1/2 & QVW-250   checkbox checkbox     checkbox     checkbox .500 3 .018 .134 checkbox checkbox checkbox checkbox checkbox checkbox checkbox checkbox checkbox
W-10S/W-15S     checkbox   checkbox         .188 .500 .020 .040 checkbox     checkbox checkbox checkbox     checkbox
WH-150   checkbox checkbox     checkbox     checkbox .375 1.500 .020 .083 checkbox checkbox checkbox checkbox checkbox checkbox checkbox checkbox checkbox
WH-200   checkbox checkbox     checkbox     checkbox .500 3.000 .020 .135 checkbox checkbox checkbox checkbox checkbox checkbox checkbox checkbox checkbox
WH-250   checkbox checkbox     checkbox     checkbox .750 3.500 .035 .180 checkbox checkbox checkbox checkbox checkbox checkbox checkbox checkbox checkbox
WH-350   checkbox checkbox     checkbox     checkbox 1.250 5.500 .065 .375 checkbox checkbox checkbox checkbox checkbox checkbox checkbox checkbox checkbox