Series/Formula Name |
Operation |
Chemistry |
Application Method |
Metal |
Cleaning
Method |
Hazardous
Materials Identification Systems (HMIS) |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
|
|
| Pro-Form 850 Emulsifiable |
 |
|
 |
 |
|
 |
|
 |
|
|
|
|
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
|
1 |
1 |
0 |
B |
| Pro-Form 855 |
|
 |
|
|
|
 |
|
 |
|
|
|
|
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
|
1 |
1 |
0 |
B |
| Pro-Form 858 |
 |
|
 |
 |
|
|
 |
 |
|
|
|
|
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
|
1 |
1 |
0 |
B |
| Pro-Form 865 |
 |
 |
 |
 |
|
|
|
|
 |
|
|
|
 |
 |
|
|
|
 |
 |
 |
 |
 |
 |
 |
|
1 |
0 |
0 |
B |
| Pro-Form 870 |
 |
|
 |
 |
|
 |
 |
|
 |
|
|
|
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
|
0 |
1 |
0 |
B |
| Pro-Form 870-15 |
|
 |
|
|
|
 |
 |
|
 |
|
|
|
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
|
0 |
1 |
0 |
B |
| Pro-Form 875 |
 |
|
 |
 |
|
 |
 |
|
 |
|
|
|
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
|
0 |
1 |
0 |
B |
| Pro-Form 805 |
|
 |
|
|
|
|
|
|
|
 |
|
|
 |
 |
 |
 |
|
 |
 |
 |
 |
 |
 |
|
|
1 |
3 |
0 |
B |
| Pro-Form 807 |
|
 |
|
|
|
|
|
|
|
 |
|
|
 |
 |
 |
 |
|
 |
|
|
|
|
 |
|
|
1 |
3 |
0 |
B |
| Pro-Form 809 |
|
 |
|
|
|
|
|
|
|
 |
|
|
 |
 |
 |
 |
|
 |
|
|
|
|
|
|
|
1 |
3 |
0 |
B |
| Pro-Form 811 |
|
 |
|
|
|
|
|
|
|
 |
|
|
 |
 |
 |
 |
|
 |
|
|
|
|
|
|
|
1 |
3 |
0 |
B |
AMCOL CORP.
Hazel Park, MI
|
| 2400 Candraw |
|
 |
 |
|
|
|
|
|
 |
|
|
|
 |
|
 |
 |
 |
 |
 |
|
|
 |
 |
 |
|
1 |
0 |
0 |
B |
| 310SST Canmist |
|
|
 |
 |
|
|
|
|
 |
|
|
|
|
 |
|
|
 |
|
|
|
|
|
|
 |
|
1 |
1 |
0 |
B |
| 4221 Canddraw |
|
|
 |
 |
|
|
 |
|
|
|
|
|
 |
 |
 |
|
|
|
|
|
|
|
|
|
|
1 |
1 |
0 |
B |
| Roll Film Vanishing Oils |
|
 |
|
|
|
|
|
|
|
 |
|
|
 |
|
 |
|
|
 |
 |
 |
 |
|
 |
|
|
2 |
2 |
0 |
G |
BENZ OIL
Milwaukee, WI
|
| Rex Draw 176 |
 |
 |
 |
 |
|
 |
 |
|
|
|
|
|
 |
|
 |
 |
|
|
|
|
 |
 |
 |
 |
 |
1 |
1 |
0 |
|
| Rex Draw 2052B |
 |
 |
 |
 |
|
|
 |
|
|
|
|
|
 |
 |
 |
|
 |
|
|
|
 |
 |
 |
 |
 |
1 |
1 |
0 |
|
| Regal Draw 336B |
 |
 |
 |
 |
|
 |
 |
|
|
|
|
|
 |
|
 |
 |
|
|
|
|
 |
 |
 |
 |
 |
1 |
1 |
0 |
|
| Vanishing Oil 122 |
|
 |
|
|
|
|
|
|
|
 |
|
|
 |
|
 |
 |
 |
|
|
 |
|
 |
|
 |
 |
1 |
2 |
1 |
|
| Vanishing Oil 122 |
|
 |
|
|
|
|
|
|
|
 |
|
|
 |
|
 |
 |
 |
|
|
 |
|
 |
|
 |
 |
1 |
2 |
1 |
|
| Vanishing Oil 226 |
|
 |
|
|
|
|
|
|
|
 |
|
|
 |
|
 |
 |
 |
|
|
 |
|
 |
|
 |
 |
1 |
2 |
1 |
|
| Vanishing Oil 667 |
|
 |
|
|
|
|
|
|
|
 |
|
|
 |
|
 |
 |
 |
 |
 |
 |
|
 |
|
 |
 |
1 |
2 |
1 |
|
| Royal Draw 746 |
|
 |
 |
|
|
|
 |
|
|
|
|
|
 |
|
 |
|
 |
 |
 |
 |
|
 |
|
 |
 |
1 |
1 |
0 |
|
| Royal Draw 749 |
|
 |
 |
|
|
|
 |
|
|
|
|
|
 |
|
 |
|
 |
 |
 |
 |
|
 |
|
 |
 |
1 |
1 |
0 |
|
BRIGHTON LABORATORIES INC.
Howell, MI
|
| Drawchem 1495 |
 |
 |
 |
 |
|
 |
|
|
|
|
|
|
 |
 |
 |
 |
 |
 |
 |
|
 |
 |
 |
 |
|
1 |
0 |
|
B |
| Drylube 1740 |
 |
 |
 |
 |
 |
|
|
|
|
|
 |
|
|
|
|
|
|
 |
 |
 |
 |
 |
 |
 |
|
1 |
0 |
0 |
B |
| Drawchem 1765 |
 |
 |
 |
|
|
|
|
|
 |
|
|
|
 |
 |
 |
 |
 |
 |
 |
|
 |
 |
|
 |
|
1 |
0 |
0 |
B |
| Drawchem 1050 |
 |
 |
 |
|
|
|
|
 |
|
|
|
|
 |
 |
 |
 |
 |
 |
 |
|
 |
 |
 |
 |
|
1 |
0 |
0 |
B |
| Drawchem VO 1228 |
|
 |
|
|
|
|
|
|
|
 |
|
|
 |
|
 |
 |
|
 |
 |
 |
 |
 |
 |
 |
|
2 |
2 |
0 |
B |
| Drawchem 1412 |
 |
 |
 |
 |
|
|
|
 |
|
|
|
|
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
|
1 |
0 |
0 |
B |
| Drawchem 1766 |
 |
 |
 |
 |
|
|
|
|
 |
|
|
|
 |
 |
 |
 |
|
 |
 |
 |
 |
 |
|
 |
|
1 |
0 |
0 |
B |
| Drawchem 1717 |
 |
 |
 |
|
|
|
|
|
 |
|
|
|
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
|
 |
|
1 |
0 |
0 |
B |
CHAIN OIL CO.
Wixom, MI
|
| Various |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
|
|
|
|
CHEMTOOL INC.
Crystal Lake, IL
|
| Lubridraw 3477 |
 |
|
 |
 |
|
|
|
|
 |
|
|
|
 |
 |
 |
 |
 |
 |
 |
|
 |
 |
 |
 |
|
1 |
0 |
0 |
B |
| Lubridraw 3417 |
|
 |
|
|
|
|
|
|
 |
|
|
|
 |
 |
 |
 |
 |
 |
 |
 |
|
 |
 |
 |
|
1 |
0 |
0 |
B |
| CT3300 |
 |
 |
 |
 |
|
 |
|
|
|
|
|
|
 |
 |
 |
 |
 |
 |
 |
 |
|
|
|
 |
|
1 |
1 |
0 |
B |
| CT3300-FE |
 |
|
 |
 |
|
 |
|
|
|
|
|
|
 |
 |
 |
 |
 |
|
|
|
 |
 |
 |
 |
|
1 |
1 |
0 |
B |
| CT3359 |
 |
|
 |
 |
|
|
 |
|
|
|
|
|
 |
 |
 |
 |
|
|
|
|
|
|
|
 |
|
1 |
1 |
0 |
B |
| CT3350 |
 |
 |
 |
 |
|
 |
|
|
|
|
|
|
 |
 |
 |
 |
|
 |
 |
 |
 |
 |
 |
 |
|
1 |
1 |
0 |
B |
| CT3340 |
 |
|
 |
 |
|
|
 |
|
|
|
|
|
 |
 |
 |
 |
|
 |
 |
 |
 |
 |
 |
 |
|
1 |
1 |
0 |
B |
| CT3425 |
|
 |
|
|
|
|
|
|
|
 |
|
|
 |
 |
 |
 |
|
 |
 |
 |
 |
 |
 |
 |
|
1 |
1 |
0 |
B |
| CT3430 |
|
 |
|
|
|
|
|
|
|
 |
|
|
 |
 |
 |
 |
|
 |
 |
 |
 |
 |
 |
 |
|
1 |
1 |
0 |
B |
| NuSol Lubriform Penultimate |
 |
 |
 |
 |
|
|
|
|
 |
|
|
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
|
1 |
0 |
0 |
B |
CONSULTANT LUBRICANTS INC.
St. Charles, MO
|
| 7901 |
 |
 |
 |
|
|
|
|
|
 |
|
|
|
 |
 |
 |
|
 |
 |
 |
 |
 |
 |
 |
 |
|
1 |
0 |
0 |
A |
| 9300 |
 |
|
 |
 |
|
 |
|
|
|
|
|
|
 |
 |
 |
 |
|
 |
 |
 |
 |
 |
 |
 |
|
1 |
1 |
0 |
A |
| 630 |
|
 |
|
|
 |
|
|
|
 |
|
|
|
|
 |
|
|
 |
 |
 |
|
 |
 |
 |
 |
|
1 |
0 |
0 |
A |
| 977 |
|
 |
|
|
|
|
|
|
|
 |
|
|
 |
 |
 |
|
 |
 |
 |
|
 |
 |
 |
|
|
1 |
2 |
0 |
B |
| 290 |
|
 |
|
|
|
 |
|
|
|
|
|
|
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
|
1 |
1 |
0 |
A |
| 703 |
|
 |
|
|
|
|
|
|
 |
|
|
|
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
|
1 |
0 |
0 |
A |
| 399 |
|
 |
 |
|
 |
|
|
|
|
|
 |
 |
|
 |
|
|
|
 |
 |
 |
 |
 |
 |
 |
|
1 |
0 |
0 |
B |
D.A. STUART CO.
Warrenville, IL
|
| Drawsol WM Series |
 |
 |
 |
 |
|
 |
|
 |
 |
|
|
|
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
|
1 |
1 |
0 |
B |
| Drawsol Neat Oils |
 |
 |
 |
 |
|
|
 |
|
|
 |
|
|
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
|
1 |
1 |
0 |
B |
| Drawsol Non-Chlorinated Neat Oils |
 |
 |
 |
 |
|
|
 |
|
|
 |
|
|
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
|
1 |
1 |
0 |
B |
| Hydroform Series |
|
|
|
 |
 |
|
|
|
|
|
 |
|
|
 |
|
|
 |
 |
 |
|
|
 |
 |
 |
|
1 |
1 |
0 |
B |
| Thermex CF Cold Heading Oils |
|
|
|
 |
|
|
 |
|
|
|
|
|
|
|
 |
 |
|
 |
 |
 |
 |
 |
 |
 |
|
1 |
1 |
0 |
B |
ETNA PRODUCTS INC.
Chagrin Falls, OH
|
| Masterdraw® 6050B |
|
 |
|
|
|
|
 |
|
|
|
|
|
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
1 |
1 |
0 |
C |
| Masterdraw® 727 |
|
 |
|
|
|
|
 |
|
|
|
|
|
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
1 |
1 |
0 |
C |
| Masterdraw® 7002HVRP |
 |
|
 |
 |
|
|
 |
|
|
|
|
|
 |
 |
 |
 |
 |
|
 |
|
 |
 |
 |
 |
 |
1 |
0 |
0 |
C |
| Masterdraw® VOL G |
|
 |
|
|
|
|
|
|
|
 |
|
|
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
1 |
3 |
0 |
C |
| Daphne AF8AU |
|
 |
|
|
|
|
|
|
|
 |
|
|
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
1 |
1 |
0 |
C |
| Masterdraw® SOL G |
|
 |
|
|
|
 |
|
|
|
|
|
|
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
|
1 |
1 |
0 |
C |
| Masterdraw® SOL H 3850 |
|
 |
|
|
|
 |
|
|
|
|
|
|
 |
 |
 |
 |
 |
|
 |
|
 |
 |
 |
 |
|
1 |
1 |
0 |
C |
| Masterdraw® SOL S 3950 |
 |
|
 |
 |
|
 |
|
|
|
|
|
|
 |
 |
 |
 |
 |
|
 |
|
 |
 |
 |
 |
|
1 |
1 |
0 |
C |
| Masterdraw® SSY G |
|
 |
|
|
|
|
|
 |
|
|
|
|
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
|
1 |
1 |
0 |
C |
| Avantin SSY H |
|
 |
 |
|
|
|
|
 |
|
|
|
|
 |
 |
 |
 |
 |
|
 |
|
 |
 |
 |
 |
|
1 |
1 |
0 |
C |
| Masterdraw® SSY S |
 |
|
 |
 |
|
|
|
 |
|
|
|
|
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
|
1 |
1 |
0 |
C |
| Masterdraw® SYN G |
|
 |
|
|
|
|
|
|
 |
|
|
|
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
|
1 |
1 |
0 |
C |
| Masterdraw® SYN H |
|
 |
 |
|
|
|
|
|
 |
|
|
|
 |
 |
 |
 |
 |
|
 |
|
 |
 |
 |
 |
|
1 |
1 |
0 |
C |
| Masterdraw® SYN S |
|
|
 |
 |
|
|
|
|
 |
|
|
|
 |
 |
 |
 |
 |
|
 |
|
 |
 |
 |
 |
|
1 |
1 |
0 |
C |
| Masterdraw® SYN S 5100 |
 |
|
 |
|
|
|
|
|
 |
|
|
|
 |
 |
 |
 |
 |
|
|
|
 |
 |
|
 |
|
1 |
0 |
0 |
C |
| Masterdraw® SYN S 5200 |
 |
|
 |
 |
|
|
|
|
 |
|
|
|
 |
 |
 |
 |
 |
|
|
|
 |
 |
|
 |
|
1 |
0 |
0 |
C |
| Masterdraw® SYN S 5300 |
 |
|
 |
 |
|
|
|
|
 |
|
|
|
 |
 |
 |
 |
 |
|
|
|
 |
 |
|
 |
|
1 |
0 |
0 |
C |
| Masterdraw® 434 |
|
 |
|
|
|
|
|
|
 |
|
|
|
 |
 |
 |
|
|
 |
 |
 |
 |
 |
 |
 |
|
1 |
0 |
0 |
C |
| Masterdraw® 417 |
|
 |
 |
|
|
|
|
|
 |
|
|
|
 |
 |
 |
|
|
 |
 |
|
 |
 |
 |
 |
|
1 |
0 |
0 |
C |
GENERAL CHEMICAL CORP.
Brighton, MI
|
| Evaplube 2200 |
|
 |
|
|
|
|
|
|
|
 |
|
|
 |
 |
 |
 |
|
 |
|
 |
 |
 |
|
 |
 |
2 |
2 |
0 |
B |
| Evaplube 2231 |
|
 |
|
|
|
|
|
|
|
 |
|
|
 |
 |
 |
 |
|
 |
|
 |
 |
 |
|
 |
 |
2 |
2 |
0 |
B |
| Evaplube 2240 |
|
 |
|
|
|
|
|
|
|
 |
|
|
 |
 |
 |
 |
|
 |
|
 |
 |
 |
|
 |
 |
2 |
2 |
0 |
B |
| Evaplube 3010 |
|
 |
|
|
|
|
|
|
|
 |
|
|
 |
 |
 |
 |
|
 |
|
 |
 |
 |
|
 |
 |
2 |
2 |
0 |
B |
| Evaplube 6460 |
|
 |
 |
|
|
|
|
|
|
 |
|
|
 |
 |
 |
 |
|
 |
|
 |
 |
 |
|
 |
 |
2 |
2 |
0 |
B |
| Gendraw 3250 |
|
|
 |
 |
|
|
|
|
 |
|
|
|
 |
 |
 |
 |
 |
 |
|
 |
 |
 |
|
 |
|
1 |
0 |
0 |
D |
| Gendraw 3520 |
|
|
 |
 |
|
|
|
|
|
 |
|
|
 |
 |
 |
 |
 |
 |
|
 |
 |
 |
|
 |
|
1 |
0 |
0 |
D |
| Gendraw 3590 |
|
|
 |
|
|
|
|
|
 |
|
|
|
 |
 |
 |
 |
 |
 |
|
 |
 |
 |
|
 |
|
1 |
0 |
0 |
D |
| Gendraw 3840 |
|
|
 |
 |
|
 |
|
|
|
|
|
|
 |
 |
 |
 |
 |
|
|
|
|
|
|
|
|
2 |
1 |
0 |
D |
| Gendraw 3850 |
 |
|
 |
 |
|
|
 |
|
|
|
|
|
 |
 |
 |
 |
|
 |
|
 |
 |
 |
|
 |
|
2 |
1 |
0 |
D |
| Gendraw 3860 |
 |
|
 |
 |
|
 |
|
|
|
|
|
|
 |
 |
 |
 |
 |
 |
|
|
 |
 |
|
 |
|
2 |
1 |
0 |
D |
| Gendraw 3920 |
 |
|
|
 |
|
 |
|
|
|
|
|
|
 |
 |
 |
 |
 |
 |
|
|
 |
 |
|
 |
|
1 |
1 |
0 |
D |
| Gendraw 3970 |
 |
|
 |
 |
|
|
|
|
 |
|
|
|
|
|
|
|
|
 |
|
 |
 |
 |
|
 |
|
1 |
0 |
0 |
D |
HANGSTERFER'S LABORATORIES INC.
Mantua, NJ
|
| Aldraw J-1 |
 |
 |
 |
 |
|
|
 |
|
|
|
|
 |
 |
 |
 |
 |
|
 |
|
 |
 |
|
|
 |
|
1 |
1 |
0 |
A |
| Aldraw J-2 |
 |
 |
 |
 |
|
|
 |
|
|
|
|
 |
 |
 |
 |
 |
|
 |
|
 |
 |
|
|
 |
|
1 |
1 |
0 |
A |
| Aldraw JD8801 |
 |
 |
 |
 |
|
|
 |
|
|
|
|
 |
|
 |
|
 |
|
 |
|
 |
 |
|
|
 |
|
1 |
1 |
0 |
A |
| Aldraw JH9402 |
 |
 |
 |
 |
|
|
 |
|
|
|
|
 |
|
 |
|
 |
|
|
|
|
 |
|
|
 |
|
1 |
1 |
0 |
A |
| Aldraw JD9020 |
 |
 |
 |
 |
|
|
|
|
 |
|
|
 |
 |
 |
 |
 |
 |
 |
|
 |
 |
|
 |
 |
|
1 |
1 |
0 |
A |
| Aldraw JD9030 |
 |
 |
 |
 |
|
|
|
|
 |
|
|
 |
 |
 |
 |
 |
|
 |
|
 |
 |
|
 |
 |
|
1 |
1 |
0 |
A |
| Hard Cut 525 |
|
 |
|
|
|
|
 |
|
|
|
|
 |
 |
 |
 |
 |
|
 |
|
 |
 |
|
|
 |
|
1 |
1 |
0 |
A |
| Hard Cut 541 |
|
 |
|
|
|
|
 |
|
|
|
|
|
 |
 |
 |
 |
 |
|
|
|
|
|
|
 |
|
1 |
1 |
0 |
A |
| S-500 |
|
|
|
 |
|
 |
|
|
|
|
|
 |
 |
 |
 |
 |
 |
|
|
 |
 |
|
 |
|
|
0 |
1 |
0 |
A |
| S-500CF |
|
 |
 |
 |
|
 |
|
|
|
|
|
 |
 |
 |
 |
 |
 |
|
|
 |
 |
|
 |
|
|
0 |
1 |
0 |
A |
| 111QDNF |
 |
|
 |
 |
 |
|
 |
|
 |
 |
|
|
|
 |
|
|
|
|
|
|
 |
 |
 |
|
|
|
|
|
|
| S600 |
 |
|
 |
|
|
 |
|
|
|
|
|
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
|
0 |
1 |
0 |
A |
| 114QDNF |
 |
|
 |
 |
 |
|
 |
|
 |
 |
|
|
|
 |
|
|
|
|
|
|
 |
 |
 |
|
|
2 |
1 |
0 |
A |
| S-800 |
 |
|
 |
 |
|
 |
|
|
|
|
|
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
|
1 |
1 |
0 |
A |
| VC 3 |
|
 |
|
|
|
 |
|
|
|
|
|
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
|
1 |
1 |
0 |
A |
| Crystal Cut 465 |
|
|
|
|
|
 |
|
|
 |
|
|
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
|
1 |
1 |
0 |
A |
HARRY MILLER CORP.
Philadelphia, PA
|
| Aqualube 2023-FR |
|
 |
|
|
|
|
|
|
 |
|
|
|
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
1 |
0 |
0 |
B |
| Hamico 138/L |
|
 |
|
|
|
|
|
|
|
 |
|
|
|
 |
 |
 |
|
|
|
 |
|
 |
|
 |
 |
1 |
2 |
0 |
B |
| Hamico 142-B |
|
 |
 |
|
|
|
|
|
|
 |
|
|
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
1 |
2 |
0 |
B |
| Hamilube 1744-EP |
|
 |
|
|
|
|
|
|
|
 |
|
|
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
1 |
2 |
0 |
B |
| Hamidraw 1945-300 |
 |
 |
|
|
|
|
 |
|
|
|
|
|
 |
 |
 |
 |
|
|
|
 |
 |
 |
 |
 |
 |
1 |
0 |
0 |
B |
| Hamidraw 1945-700 |
 |
|
 |
|
|
|
 |
|
|
|
|
|
 |
 |
 |
 |
|
|
|
 |
 |
 |
|
 |
 |
1 |
0 |
0 |
B |
| Hamidraw 6301 (Nonchlorinated) |
|
|
|
|
|
|
 |
|
|
|
|
|
 |
 |
 |
 |
|
|
|
|
 |
 |
 |
 |
 |
1 |
0 |
0 |
B |
| Hamilube 2078-B |
 |
|
 |
 |
|
 |
|
|
|
|
|
|
 |
 |
 |
 |
|
|
|
 |
 |
 |
 |
 |
 |
1 |
0 |
0 |
B |
| Hamilube 2080 |
 |
|
 |
|
|
|
 |
|
|
|
|
|
 |
 |
 |
 |
|
 |
 |
|
|
|
|
 |
 |
1 |
0 |
0 |
B |
| Hamidraw 2080-B |
 |
 |
 |
|
|
|
 |
|
|
|
|
|
 |
 |
 |
 |
 |
 |
|
|
|
|
|
 |
 |
1 |
0 |
0 |
B |
| Hamidraw 1846-B |
|
|
|
 |
|
|
 |
|
|
|
|
|
|
 |
 |
 |
|
|
|
|
 |
 |
|
 |
|
1 |
0 |
0 |
A |
| Hamidraw 497-B |
 |
|
 |
|
|
|
 |
|
|
|
|
|
 |
 |
 |
 |
|
|
|
 |
 |
 |
|
 |
 |
1 |
1 |
0 |
B |
| Hamilube 9200-VP |
|
 |
|
|
|
|
 |
|
|
|
|
|
 |
 |
 |
 |
|
|
|
 |
 |
 |
|
 |
 |
1 |
0 |
0 |
B |
| Hamidraw 1828-LC |
 |
|
 |
|
|
 |
|
|
|
|
|
|
 |
 |
 |
 |
 |
|
|
 |
 |
 |
|
 |
 |
1 |
1 |
0 |
B |
| Hamidraw 9000-F (Nonchlorinated) |
 |
 |
 |
|
|
 |
|
|
|
|
|
|
 |
 |
 |
 |
 |
|
|
 |
 |
 |
 |
 |
 |
1 |
1 |
0 |
B |
| Hamidraw 1828-A |
 |
|
|
 |
|
 |
|
|
|
|
|
|
 |
 |
 |
 |
 |
|
|
 |
 |
 |
|
 |
 |
1 |
1 |
0 |
B |
| Hamidraw 1829 |
 |
|
|
 |
|
 |
|
|
|
|
|
|
 |
 |
 |
 |
 |
|
|
 |
 |
 |
|
 |
 |
1 |
0 |
0 |
B |
HOUGHTON INTL. INC.
Valley Forge, PA
|
| Cindol 2822 |
|
 |
|
|
|
 |
|
|
|
 |
|
 |
 |
 |
 |
 |
 |
 |
|
|
|
 |
 |
 |
|
1 |
1 |
0 |
B |
| Cindol 4612 |
|
 |
|
|
 |
|
|
|
|
 |
|
 |
 |
 |
 |
 |
 |
 |
 |
 |
|
 |
 |
 |
 |
1 |
1 |
0 |
B |
| Cindol 4689 |
 |
 |
 |
|
|
|
 |
|
|
|
|
 |
 |
 |
 |
 |
 |
 |
 |
 |
|
 |
 |
 |
 |
1 |
1 |
0 |
B |
| Houghto-Draw 404 |
 |
|
 |
 |
|
|
 |
|
|
|
|
|
 |
 |
 |
 |
|
 |
|
|
|
 |
|
 |
 |
1 |
1 |
0 |
B |
| Houghto-Draw 7002 |
 |
 |
 |
|
|
 |
|
|
|
|
|
|
 |
 |
 |
 |
 |
 |
|
|
|
 |
 |
 |
|
1 |
1 |
0 |
B |
| Houghto-Draw 7047-EP |
 |
 |
|
|
|
|
|
|
 |
|
|
 |
 |
 |
 |
 |
 |
 |
 |
 |
|
 |
 |
 |
|
1 |
1 |
0 |
B |
| Houghto-Draw 7066 |
 |
 |
|
|
|
 |
|
|
|
|
|
 |
 |
 |
 |
 |
 |
 |
 |
 |
|
 |
 |
 |
|
1 |
1 |
0 |
B |
| Houghto-Draw 7077 |
 |
 |
 |
 |
|
 |
|
|
|
|
|
 |
 |
 |
 |
 |
 |
 |
|
|
 |
 |
|
 |
|
1 |
1 |
0 |
B |
| Houghto-Prep 7079-R |
 |
 |
 |
 |
|
 |
|
|
|
|
|
 |
 |
 |
 |
 |
 |
 |
|
|
 |
 |
|
 |
|
1 |
1 |
0 |
B |
| Houghto-Draw 7091 |
 |
 |
 |
|
|
|
 |
|
|
|
|
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
1 |
1 |
0 |
B |
| Houghto-Draw PF 100 |
 |
 |
 |
 |
|
 |
|
|
|
|
|
 |
 |
 |
 |
 |
 |
 |
|
|
 |
 |
|
 |
|
1 |
1 |
0 |
B |
| Houghto-Draw TC 100 |
 |
 |
|
|
|
|
|
|
 |
|
|
 |
 |
 |
 |
 |
 |
 |
 |
 |
|
 |
 |
 |
|
1 |
1 |
0 |
B |
| Houghto-Draw WD 4814 |
|
 |
|
|
|
 |
|
|
|
|
|
 |
|
 |
 |
 |
 |
 |
|
 |
|
|
|
 |
|
1 |
1 |
0 |
B |
| SHO 707 |
 |
 |
 |
 |
|
|
 |
|
|
|
|
 |
 |
 |
 |
 |
 |
 |
|
|
 |
 |
|
 |
 |
1 |
1 |
0 |
B |
INTERNATIONAL CHEMICAL CO.
Philadelphia, PA
|
| I.C. 1599 |
 |
|
|
 |
|
|
|
|
 |
|
|
|
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
|
1 |
0 |
0 |
D |
| I.C. 2502 |
|
 |
|
|
|
|
|
|
 |
|
|
|
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
|
1 |
0 |
0 |
D |
| I.C. 2504 |
 |
|
|
 |
|
|
|
|
 |
|
|
|
 |
 |
 |
 |
 |
|
|
|
 |
 |
|
 |
|
1 |
0 |
0 |
D |
| I.C. 1598 |
|
 |
|
|
|
|
|
|
 |
|
|
|
 |
 |
 |
 |
 |
 |
 |
 |
|
 |
|
 |
|
1 |
0 |
0 |
D |
| I.C. 1576 |
|
 |
|
|
|
|
|
|
 |
|
|
 |
 |
|
|
|
|
 |
 |
|
 |
 |
|
 |
|
1 |
0 |
0 |
D |
| I.C. 2801 Series |
 |
 |
 |
 |
|
|
|
 |
|
|
|
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
|
1 |
1 |
0 |
C |
| I.C. 920-R |
 |
|
|
 |
|
 |
|
|
|
|
|
|
 |
 |
 |
 |
 |
 |
 |
|
 |
 |
|
 |
|
2 |
1 |
0 |
C |
| I.C. 1211 Series |
 |
 |
 |
 |
|
|
 |
|
|
|
|
|
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
|
1 |
1 |
0 |
B |
| I.C. 848 Series |
|
 |
|
|
|
|
|
|
|
 |
|
|
 |
 |
 |
 |
|
 |
 |
 |
|
 |
 |
 |
|
2 |
2 |
0 |
D |
| I.C. 345 |
 |
|
 |
|
|
|
|
 |
|
|
|
|
 |
 |
|
|
|
 |
 |
 |
 |
 |
 |
 |
|
0 |
0 |
0 |
B |
| I.C. 126-B |
 |
|
|
 |
 |
|
|
|
|
|
 |
|
|
|
|
|
|
 |
 |
|
 |
 |
 |
 |
|
2 |
0 |
0 |
E |
| I.C. 152 |
|
 |
|
|
|
|
|
|
|
 |
 |
|
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
|
 |
2 |
1 |
0 |
D |
| Rolleze 2500 |
 |
 |
 |
 |
|
|
|
|
 |
|
|
|
 |
 |
 |
 |
|
 |
 |
 |
 |
 |
 |
 |
|
1 |
0 |
0 |
E |
| Pre-Lube 2801-DL |
|
 |
 |
|
 |
|
|
 |
|
|
|
 |
|
|
|
|
|
 |
|
 |
 |
 |
 |
 |
 |
1 |
0 |
0 |
D |
IRMCO LEANGREEN METALFORMING
Evanston, IL
|
| IRMCO FLUIDS ® |
 |
 |
 |
 |
|
|
|
|
 |
|
|
|
 |
 |
|
|
 |
 |
 |
 |
 |
 |
 |
 |
|
1 |
0 |
0 |
|
| IRMCO FLUIDS ® High-strength Steel Formula |
 |
 |
 |
 |
|
|
|
|
 |
|
|
|
 |
 |
|
|
 |
|
|
|
 |
 |
|
 |
|
1 |
0 |
0 |
|
| IRMCO GEL® IRMCO EXTREME® Advanced Tube Forming Films |
|
 |
|
|
|
|
|
|
 |
|
|
|
|
|
|
|
|
 |
 |
 |
 |
 |
 |
 |
|
1 |
0 |
0 |
|
ITW ROCOL NORTH AMERICA
Glenview, IL
|
| Accu-Lube PowerStamp II |
 |
 |
 |
 |
|
|
 |
|
|
|
|
|
 |
 |
 |
|
 |
 |
 |
 |
 |
 |
 |
 |
|
0 |
1 |
0 |
B |
| Accu-Lube PowerStamp III |
 |
 |
 |
 |
|
|
 |
|
|
|
|
|
 |
 |
 |
|
 |
 |
 |
 |
 |
 |
 |
 |
|
0 |
1 |
0 |
B |
| Metal Mates VS 160-3 |
 |
 |
 |
 |
|
|
|
 |
|
|
|
|
 |
 |
 |
 |
 |
 |
 |
|
 |
 |
 |
 |
|
1 |
1 |
0 |
B |
| Metal Mates OVS 210-21 |
 |
 |
 |
 |
|
|
|
 |
|
|
|
|
 |
 |
 |
 |
 |
 |
 |
|
 |
 |
 |
 |
|
1 |
1 |
0 |
B |
| Metal Mates HDP 970-40 |
 |
 |
 |
 |
|
|
|
 |
|
|
|
|
 |
 |
 |
 |
 |
 |
 |
|
 |
 |
 |
 |
|
1 |
1 |
0 |
B |
LEANDER & CO.
Ballwin, MO
|
| Chlorinate Soluble Oil 305 |
 |
 |
 |
 |
|
 |
|
|
|
|
|
|
 |
 |
 |
 |
 |
 |
 |
|
 |
 |
 |
 |
|
1 |
1 |
0 |
A |
| Chlorinated Soluble Oil 330 |
 |
 |
 |
 |
|
 |
|
|
|
|
|
|
 |
 |
 |
 |
 |
|
|
|
 |
 |
 |
 |
|
1 |
1 |
0 |
A |
| Chlorine-Free Soluble Oil 340 |
 |
 |
 |
 |
|
 |
|
|
|
|
|
|
|
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
|
1 |
1 |
0 |
A |
| Drawing Fluid 2210 |
 |
 |
 |
 |
|
|
|
|
 |
|
|
|
 |
 |
 |
 |
 |
|
|
|
 |
 |
|
 |
|
1 |
1 |
0 |
A |
| Drawing Fluid 2205 |
 |
 |
 |
 |
|
|
|
|
 |
|
|
|
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
|
1 |
0 |
0 |
A |
| Drawing Fluid 6420 |
 |
 |
 |
 |
|
|
|
|
 |
|
|
|
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
|
1 |
0 |
0 |
A |
| Vanishing Oil 101 |
|
 |
|
|
|
|
|
|
|
 |
|
|
 |
 |
 |
|
 |
 |
 |
 |
|
|
 |
|
 |
1 |
1 |
0 |
A |
| Vanishing Fluid 2261 |
|
 |
|
|
|
|
|
|
 |
|
|
|
 |
 |
 |
 |
 |
 |
 |
 |
|
|
 |
 |
|
1 |
0 |
0 |
A |
| Drawing Fluid 2230 |
|
 |
|
|
|
|
|
 |
|
|
|
|
 |
|
|
|
 |
 |
 |
 |
|
|
 |
 |
|
1 |
0 |
0 |
A |
| Drawing Oil 100 |
 |
 |
 |
 |
|
|
 |
|
|
|
|
|
 |
 |
 |
 |
 |
|
|
|
 |
 |
|
 |
|
1 |
1 |
0 |
A |
| Drawing Oil 231 |
 |
 |
 |
 |
|
|
 |
|
|
|
|
|
 |
|
|
|
 |
|
|
|
 |
 |
|
 |
 |
1 |
1 |
0 |
A |
| Dry Film 40 |
|
|
 |
|
 |
|
|
|
|
|
 |
|
 |
|
|
|
 |
 |
 |
 |
 |
 |
 |
 |
|
1 |
0 |
0 |
A |
| Dry Film 60 |
 |
 |
 |
 |
 |
|
|
|
 |
|
 |
 |
|
|
|
|
|
 |
 |
 |
 |
 |
 |
 |
|
1 |
0 |
0 |
A |
METALLOID CORP.
Huntington, IN
|
| METCHEM 552 |
|
 |
|
|
|
|
|
|
 |
|
|
|
 |
 |
 |
 |
 |
|
|
|
|
 |
|
 |
|
1 |
0 |
0 |
B |
| METCHEM 557 |
|
 |
 |
|
|
|
|
|
 |
|
|
|
 |
 |
 |
 |
 |
|
|
|
 |
 |
|
 |
|
1 |
0 |
0 |
B |
| METCHEM 604 |
|
 |
|
|
|
|
|
|
 |
|
|
|
 |
 |
 |
 |
 |
 |
 |
 |
|
 |
 |
 |
|
1 |
0 |
0 |
B |
| METCHEM 623 |
|
 |
 |
|
|
|
|
|
 |
|
|
|
 |
 |
 |
 |
 |
|
 |
 |
 |
 |
 |
 |
|
1 |
0 |
0 |
B |
| METCHEM 781 |
 |
|
 |
 |
|
|
|
|
 |
|
|
|
 |
 |
 |
 |
 |
|
|
|
 |
 |
|
 |
|
1 |
0 |
0 |
B |
| METCHEM 1015 |
 |
|
 |
 |
|
|
|
|
 |
|
|
|
 |
 |
 |
 |
 |
|
|
|
 |
 |
|
 |
|
1 |
0 |
0 |
B |
| METDRAW 407 |
|
 |
 |
|
|
|
 |
|
|
|
|
|
 |
 |
 |
 |
 |
 |
 |
|
 |
 |
 |
 |
 |
1 |
1 |
0 |
B |
| METDRAW 436 |
 |
|
 |
 |
|
|
 |
|
|
|
|
|
 |
 |
 |
 |
 |
|
|
|
 |
 |
|
|
 |
1 |
1 |
0 |
B |
| METDRAW 446 |
|
 |
 |
|
|
|
 |
|
|
|
|
|
 |
 |
 |
 |
 |
 |
 |
|
|
 |
 |
 |
 |
1 |
1 |
0 |
B |
| METDRAW 528 |
|
 |
|
|
|
|
|
|
|
 |
|
|
 |
 |
 |
 |
|
 |
 |
 |
|
 |
 |
|
|
1 |
2 |
0 |
B |
| METDRAW 534 |
|
 |
|
|
|
|
|
|
|
 |
|
|
 |
 |
 |
 |
|
 |
 |
 |
|
 |
 |
 |
|
1 |
2 |
0 |
B |
| METDRAW 541 |
|
 |
 |
 |
|
 |
|
|
|
|
|
|
 |
 |
 |
 |
 |
 |
 |
|
 |
 |
|
 |
|
1 |
1 |
0 |
B |
| METDRAW 560 |
 |
|
 |
 |
|
|
 |
|
|
|
|
|
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
|
1 |
1 |
0 |
B |
| METDRAW 609 |
|
 |
|
|
|
|
 |
|
|
|
|
|
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
|
|
1 |
1 |
0 |
B |
| METDRAW 614 |
 |
|
 |
 |
|
 |
|
|
|
|
|
|
 |
 |
 |
 |
 |
 |
 |
|
 |
 |
|
 |
|
1 |
1 |
0 |
B |
| METDRAW 688 |
|
 |
|
|
|
|
|
|
|
 |
|
|
 |
 |
 |
 |
|
 |
 |
 |
 |
 |
 |
 |
|
1 |
2 |
0 |
B |
| METDRAW 879 |
 |
|
 |
 |
|
 |
|
|
|
|
|
|
 |
 |
 |
 |
 |
|
|
|
 |
 |
|
 |
|
1 |
1 |
0 |
B |
| METSOL 606 |
|
 |
|
|
|
 |
|
|
|
|
|
|
 |
 |
 |
 |
 |
 |
 |
|
|
 |
 |
 |
|
1 |
1 |
0 |
B |
| MULTI-SLIDE 21 |
|
 |
|
|
|
|
 |
|
|
|
|
|
 |
 |
 |
 |
 |
|
 |
 |
 |
 |
 |
 |
|
1 |
1 |
0 |
B |
MILACRON INC.
Cincinnati, OH
|
| Milform 950 |
|
 |
|
|
|
|
|
|
 |
|
|
|
 |
 |
 |
 |
 |
|
|
|
 |
 |
|
 |
|
1 |
0 |
0 |
|
| Milform 1200 |
|
 |
|
|
|
|
|
|
 |
|
|
|
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
|
1 |
0 |
0 |
|
| Milform 6265 |
|
 |
|
|
|
|
|
|
 |
|
|
|
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
|
1 |
0 |
0 |
|
| Milform 6276 |
|
 |
|
|
|
|
|
|
 |
|
|
|
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
|
1 |
0 |
0 |
|
| Milform 635 |
 |
|
 |
|
|
 |
|
|
|
|
|
|
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
|
1 |
1 |
0 |
|
| Milform 64SST |
 |
|
 |
|
|
 |
|
|
|
|
|
|
 |
 |
 |
 |
 |
 |
 |
|
 |
 |
 |
 |
|
1 |
1 |
0 |
|
| Milform 6670 |
|
|
 |
|
|
|
|
|
 |
|
|
|
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
|
1 |
0 |
0 |
|
| Mildraw 6985 |
|
 |
|
|
|
|
|
|
 |
|
|
|
 |
 |
 |
 |
 |
 |
|
|
|
 |
 |
 |
|
1 |
0 |
0 |
|
| Milform 8050 |
 |
|
 |
|
|
|
|
|
 |
|
|
|
 |
 |
 |
 |
 |
 |
 |
 |
|
 |
 |
 |
|
1 |
0 |
0 |
|
| Milform 8060 |
 |
|
 |
|
|
|
|
|
 |
|
|
|
 |
 |
 |
 |
 |
 |
 |
|
|
 |
 |
 |
|
1 |
0 |
0 |
|
| Milform 7AL |
|
 |
|
|
|
|
 |
|
|
|
|
|
 |
 |
 |
 |
 |
 |
 |
 |
|
 |
|
 |
 |
1 |
1 |
0 |
|
| Mildraw 04M |
|
 |
|
|
|
|
 |
|
|
|
|
|
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
1 |
1 |
0 |
|
| Mildraw 41FB |
 |
|
|
 |
|
|
 |
|
|
|
|
|
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
1 |
1 |
0 |
|
| Milform 50 |
 |
|
|
 |
|
|
 |
|
|
|
|
|
 |
 |
 |
 |
 |
 |
 |
|
|
 |
|
 |
 |
1 |
1 |
0 |
|
| Mildraw 03V |
|
 |
|
|
|
|
|
|
|
 |
|
|
 |
 |
 |
 |
|
 |
 |
 |
 |
 |
 |
|
|
1 |
2 |
0 |
|
| Mildraw 36V |
|
 |
|
|
|
|
|
|
|
 |
|
|
 |
 |
 |
 |
|
 |
 |
 |
 |
 |
 |
|
|
1 |
2 |
0 |
|
MS FLUID TECHNOLOGIES
Indianapolis, IN
|
| Eco Draw HVE-1 (automotive-approved) |
 |
 |
|
 |
|
|
|
|
 |
|
|
|
 |
 |
 |
 |
 |
 |
 |
|
 |
 |
 |
 |
|
1 |
0 |
0 |
B |
| Eco Draw HVE-1P |
 |
 |
 |
 |
|
|
|
|
 |
|
|
|
 |
 |
 |
 |
 |
 |
 |
|
 |
 |
 |
 |
|
1 |
0 |
0 |
B |
| Eco Draw HVE-AM |
 |
 |
|
 |
|
|
|
|
 |
|
|
|
 |
 |
 |
 |
 |
 |
 |
|
 |
 |
 |
 |
|
1 |
0 |
0 |
B |
| Eco Draw HVRG |
 |
|
 |
 |
|
|
|
|
 |
|
|
|
 |
|
 |
 |
 |
|
 |
|
 |
 |
 |
 |
|
1 |
0 |
0 |
B |
| Eco Draw HVPX |
 |
|
 |
 |
|
|
|
|
 |
|
|
|
 |
 |
 |
 |
 |
|
|
|
 |
 |
|
 |
|
1 |
0 |
0 |
B |
| Eco Draw XL75 |
 |
|
 |
 |
|
|
|
|
 |
|
|
|
 |
 |
 |
 |
 |
|
|
|
 |
 |
|
 |
|
1 |
0 |
0 |
B |
| Eco Gel 28 |
|
 |
 |
|
|
|
|
|
 |
|
|
 |
 |
|
 |
|
|
|
|
|
 |
 |
|
 |
|
1 |
0 |
0 |
B |
| Eco Lube BR |
|
 |
|
|
|
|
|
|
 |
|
|
|
|
|
|
|
|
|
|
 |
|
|
|
 |
|
1 |
0 |
0 |
B |
| XL Draw K |
 |
 |
 |
 |
|
 |
|
|
|
|
|
|
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
|
1 |
1 |
0 |
B |
| XL Draw RX |
 |
 |
 |
 |
|
 |
|
|
|
|
|
|
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
|
1 |
1 |
0 |
B |
| XL Draw 7000 |
 |
 |
 |
 |
|
|
|
 |
|
|
|
|
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
|
1 |
1 |
0 |
B |
| XL Draw WI |
 |
|
 |
 |
|
|
 |
|
|
|
|
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
|
1 |
1 |
0 |
B |
| Dri Coat |
 |
 |
 |
 |
 |
|
|
|
 |
|
 |
|
 |
|
|
|
|
|
|
|
 |
 |
|
 |
|
1 |
0 |
0 |
B |
| Hot Melt NR |
 |
|
 |
 |
 |
|
|
 |
|
|
 |
|
 |
|
|
|
|
 |
 |
|
 |
 |
 |
 |
|
1 |
1 |
0 |
B |
| Forming Oil 5005 |
 |
 |
 |
|
|
|
 |
|
|
|
|
|
|
|
|
|
 |
 |
 |
 |
 |
 |
 |
 |
 |
1 |
1 |
0 |
B |
OAK INTL.
Sturgis, MI
|
| Oakform DSY 6150 |
|
 |
|
|
|
|
|
|
 |
|
|
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
|
1 |
0 |
0 |
|
| Oakform DSY 6250 |
|
 |
|
|
|
|
|
|
 |
|
|
 |
 |
 |
 |
 |
 |
|
|
|
 |
 |
 |
 |
|
1 |
0 |
0 |
|
| Oakform DSY 6500 |
|
 |
|
|
|
|
|
|
 |
|
|
 |
 |
 |
 |
 |
 |
 |
 |
|
|
 |
 |
 |
|
1 |
0 |
0 |
|
| Oakform DSY 6551 |
|
 |
|
|
|
|
|
|
 |
|
|
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
|
1 |
0 |
0 |
|
| Oakform DSY 6553 |
|
|
 |
|
|
|
|
|
 |
|
|
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
|
1 |
0 |
0 |
|
| Oakform DSY 7250 |
 |
|
 |
|
|
|
|
|
 |
|
|
 |
 |
 |
 |
 |
 |
 |
 |
|
|
 |
 |
 |
|
1 |
0 |
0 |
|
| Oakform DSS 6900HD |
 |
|
 |
|
|
|
|
 |
|
|
|
 |
 |
 |
 |
 |
 |
 |
 |
|
 |
 |
 |
 |
|
1 |
1 |
0 |
|
| Oakform DSO 6600 |
 |
|
 |
|
|
 |
|
|
|
|
|
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
|
1 |
1 |
0 |
|
| Oakform DSO 6800HD |
 |
|
 |
|
|
 |
|
|
|
|
|
 |
 |
 |
 |
 |
 |
 |
 |
|
 |
 |
 |
 |
|
1 |
1 |
0 |
|
| Oakform DST 6400FB |
 |
|
|
 |
|
|
 |
|
|
|
|
 |
 |
 |
|
|
|
|
|
|
 |
 |
|
|
|
1 |
1 |
0 |
|
| Oak Draw 503 |
|
 |
|
|
|
|
|
|
|
 |
|
|
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
|
|
1 |
2 |
0 |
|
| Oak Draw 505 |
|
 |
|
|
|
|
|
|
|
 |
|
|
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
|
|
1 |
2 |
0 |
|
| Oak Draw 512 |
|
 |
|
|
|
|
|
|
|
 |
|
|
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
|
|
1 |
2 |
0 |
|
| Oak Draw 519 |
|
 |
|
|
|
|
|
|
|
 |
|
|
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
|
|
1 |
2 |
0 |
|
| Oak Draw 528 |
|
|
 |
|
|
|
|
|
|
 |
|
|
 |
 |
 |
 |
 |
 |
 |
|
 |
 |
|
|
|
1 |
2 |
0 |
|
| Oak Draw 536 |
|
|
 |
|
|
|
|
|
|
 |
|
|
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
|
|
1 |
2 |
0 |
|
| Oak Draw 704 |
 |
|
 |
|
|
|
|
|
 |
|
|
|
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
|
1 |
0 |
0 |
|
| Oak Draw 734 |
|
 |
|
|
|
|
|
|
 |
|
|
|
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
|
1 |
0 |
0 |
|
| Oak Draw 905 |
|
 |
|
|
|
|
 |
|
|
|
|
|
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
|
1 |
1 |
0 |
|
| Oak FB-937-A (Fineblank) |
|
|
|
 |
|
|
 |
|
|
|
|
|
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
|
2 |
1 |
0 |
|
PERKINS PRODUCTS INC.
Bedford Park, IL
|
| Perdraw 1043 |
|
 |
|
|
|
|
|
|
|
 |
|
|
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
1 |
2 |
0 |
B |
| Perdraw 1044-D |
|
 |
|
|
|
|
|
|
|
 |
|
|
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
1 |
2 |
0 |
B |
| Perdraw 1048 |
|
 |
|
|
|
|
|
|
|
 |
|
|
 |
 |
|
|
 |
 |
 |
 |
 |
 |
 |
|
 |
1 |
2 |
0 |
B |
| Perdraw 1085 |
|
 |
 |
|
|
|
|
|
|
 |
|
|
 |
 |
|
|
 |
 |
 |
 |
 |
 |
 |
|
 |
1 |
2 |
0 |
B |
| Perdraw 2510 |
|
 |
 |
 |
|
|
 |
|
|
|
|
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
1 |
1 |
0 |
A |
| Perdraw 3518 |
 |
 |
 |
 |
|
|
 |
|
|
|
|
 |
 |
 |
 |
 |
 |
|
|
|
 |
 |
|
|
 |
1 |
1 |
0 |
A |
| Perdraw 3561 |
 |
|
 |
 |
|
|
 |
|
|
|
|
|
 |
 |
 |
 |
|
|
|
|
 |
 |
 |
 |
 |
1 |
1 |
0 |
B |
| Perdraw 6270 |
|
 |
 |
 |
|
|
|
|
 |
|
|
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
|
 |
|
1 |
0 |
0 |
A |
| Perdraw 6272 |
|
 |
 |
 |
|
|
|
|
 |
|
|
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
|
 |
|
1 |
0 |
0 |
A |
| Perdraw 6298 |
 |
 |
 |
 |
|
|
|
|
 |
|
|
|
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
|
1 |
0 |
0 |
B |
| Perdraw 6288 |
 |
 |
 |
 |
|
|
|
|
 |
|
|
|
 |
 |
|
 |
 |
 |
 |
 |
 |
 |
 |
 |
|
1 |
0 |
0 |
A |
| Perdraw 6995 |
 |
 |
 |
 |
 |
|
|
|
|
|
 |
 |
 |
 |
 |
|
 |
|
|
|
 |
 |
 |
 |
|
1 |
0 |
0 |
B |
| Perkool 4121-SY |
|
 |
 |
 |
|
|
|
 |
|
|
|
 |
 |
 |
 |
 |
 |
|
|
|
 |
 |
|
 |
|
1 |
0 |
0 |
A |
| Perkool 9500-EP |
|
 |
 |
|
|
 |
|
|
|
|
|
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
1 |
1 |
0 |
A |
| Perdraw 9932-L |
 |
 |
 |
 |
|
 |
|
|
|
|
|
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
1 |
1 |
0 |
A |
| Perdraw 9932M |
 |
 |
 |
 |
|
 |
|
|
|
|
|
|
 |
 |
 |
 |
|
 |
 |
 |
 |
 |
 |
 |
|
1 |
0 |
0 |
B |
| Perdraw 7308 |
 |
 |
 |
 |
|
|
 |
|
|
|
|
|
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
|
 |
1 |
1 |
0 |
A |
PETRONOMICS MANUFACTURING GROUP INC.
Hutchinson, KS
|
| Metalpro Alpha 52199 |
 |
 |
 |
 |
|
|
 |
|
|
|
|
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
|
1 |
1 |
0 |
|
| Metalpro Beta 52204 |
 |
 |
 |
 |
|
|
 |
|
|
|
|
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
|
|
1 |
1 |
0 |
|
| Metalform 2000 52190 |
 |
 |
 |
 |
|
|
 |
|
|
|
|
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
|
|
1 |
1 |
0 |
|
| Metalform 2000-HD 52190 |
 |
 |
 |
 |
|
|
 |
|
|
|
|
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
|
|
1 |
1 |
0 |
|
| Concentrate Synthetic Mist Lube 55585 |
 |
 |
 |
 |
|
|
|
|
 |
|
|
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
|
|
1 |
1 |
0 |
|
| Metalform 3000-P 55610 |
 |
 |
 |
 |
|
|
 |
|
|
|
|
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
|
|
1 |
1 |
0 |
|
| Metalform 4000-P 55655 |
 |
 |
 |
 |
|
|
 |
|
|
|
|
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
|
|
1 |
1 |
0 |
|
| Metalform 6000 52215 |
 |
 |
 |
 |
|
|
 |
|
|
|
|
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
|
|
1 |
1 |
0 |
|
| Metalform 7000 52232 |
 |
 |
 |
 |
|
|
 |
|
|
|
|
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
|
|
1 |
1 |
0 |
|
| Synthetic Drawing & Stamping Compound 55661 |
 |
 |
 |
 |
|
|
|
|
 |
|
|
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
|
|
1 |
1 |
0 |
|
| Heavy-duty Synthetic Drawing & Stamping Compound 55666 |
 |
 |
 |
 |
|
|
|
|
 |
|
|
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
|
|
1 |
1 |
0 |
|
| Mist Lube Light-duty 55570 |
|
 |
|
|
|
|
 |
|
|
|
|
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
|
|
1 |
0 |
0 |
|
| Mist Lube Heavy-duty 55575 |
 |
|
 |
 |
|
|
 |
|
|
|
|
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
|
|
1 |
1 |
0 |
|
| Synthetic Mist Lube 55580 |
 |
 |
 |
 |
|
|
|
|
 |
|
|
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
|
|
1 |
1 |
0 |
|
| Concentrate Mist Lube 55792 |
 |
 |
 |
 |
|
|
 |
|
|
|
|
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
|
|
1 |
1 |
0 |
|
| Enviro-Stamping & Drawing Compound 55642 |
 |
 |
 |
 |
|
|
|
|
 |
|
|
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
|
0 |
0 |
0 |
|
| Semisynthetic Drawing & Stamping Compound 55670 |
 |
 |
 |
 |
|
|
|
 |
|
|
|
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
|
|
1 |
1 |
0 |
|
| Industrial Super Lube 12845 |
 |
 |
 |
 |
|
|
 |
|
|
|
|
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
|
|
1 |
1 |
0 |
|
PICO CHEMICAL CORP.
Chicago Heights, IL
|
| PICODRAW 4030 |
 |
 |
 |
|
|
|
|
|
 |
|
|
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
|
1 |
0 |
0 |
1 |
| PICODRAW 5272 |
 |
 |
 |
|
|
|
|
|
 |
|
|
 |
 |
 |
 |
 |
 |
|
|
|
 |
 |
 |
 |
|
1 |
0 |
0 |
1 |
| PICOSOL 5382 |
|
 |
 |
|
|
 |
|
|
|
|
|
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
|
1 |
1 |
0 |
1 |
| PICOEXTRUD |
|
 |
 |
|
|
|
 |
|
|
|
|
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
1 |
1 |
0 |
1 |
| PICOFORM 4700 |
|
 |
|
|
|
|
|
|
|
 |
|
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
1 |
2 |
0 |
1 |
| PICOSPIN 4016 |
 |
 |
|
|
|
|
|
|
 |
|
|
 |
 |